MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Material Category Search

Find a Material Category:
Select a Material Category: Selected Material Category:
  Search Results
There are 105 materials in the category Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced. If your material is not listed, please refer to our search strategy page for assistance in limiting your search.

Found 105 Results -- Page of 3 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
 2A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
 3DiscontinuedCovestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled
 4Bada BADAFLEX® TPU 65D 8113 GF20 natural TPU, 20% Glass Fiber Reinforced
 5BASF Elastollan® R 1001 10% Glass Filled TPUR
 6BASF Elastollan® R 1000 20% Glass Filled TPUR
 7BASF Elastollan® R 2000 20% Glass Filled TPUR
 8BASF Elastollan® R 3000 20% Glass Filled TPUR
 9BASF Elastollan® R 2001 20% Glass Filled TPUR
 10BASF Elastollan® R 2005/1 20% Glass Filled TPUR
 11BASF Elastollan® R 2006 20% Glass Filled TPUR
 12BASF Elastollan® R 2002 25% Glass Filled TPUR
 13BASF Elastollan® R 3001 15% Glass Filled TPUR
 14Envalior TEPEX® dynalite 108-FGAL290(1)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
 15Envalior TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
 16Envalior TEPEX® dynalite 108-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate
 17DiscontinuedClariant Renol PURSP0005 Polyurethane Elastomer, Glass Fiber Reinforced
 18Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin
 19Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin
 20Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin
 21Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin
 22Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin
 23Fulcrum Composites Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Strip
 24Fulcrum Composites Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod
 25GRECO ISOPAK® 8102LGF40 TPU, Long Glass Fiber Reinforced
 26GRECO ISOPAK® 8102LGF50 TPU, Long Glass Fiber Reinforced
 27GRECO ISOPAK® 8102LGF60 TPU, Long Glass Fiber Reinforced
 28GRECO ISOPAK® 8101LGF60 TPU, Long Glass Fiber Reinforced
 29GRECO ISOPAK® 8102LGF30 TPU, Long Glass Fiber Reinforced
 30DiscontinuedAvient Edgetek® UR-20GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 20% Glass Fiber Reinforced
 31DiscontinuedAvient Edgetek® UR-30GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 30% Glass Fiber Reinforced
 32Celanese Celstran® TPU-CF40-01 TPU, 40% Specialty
 33Celanese Celstran® TPU-GF30-01-US TPU, 30% Glass Reinforced
 34Celanese Celstran® TPU-GF40-01-US TPU, 40% Glass Reinforced
 35Celanese Celstran® TPU-GF50-01-US TPU, 50% Glass Reinforced
 36Celanese Celstran® TPU-GF60-01-US TPU, 60% Glass Reinforced
 37Toyobo Celstran® TPU-GF30-01 AD3002 Black TPU, 30% Long Glass Reinforced
 38Toyobo Celstran® TPU-GF30-01 AF3001 Natural TPU, 30% Long Glass Reinforced
 39Toyobo Celstran® TPU-GF40-01 AD3002 Black TPU, 40% Long Glass Reinforced
 40Toyobo Celstran® TPU-GF40-01 AF3001 Natural TPU, 40% Long Glass Reinforced
 41Toyobo Celstran® TPU-GF40-04 AF3001 Natural TPU, 40% Long Glass Reinforced
 42Toyobo Celstran® TPU-GF50-01 AD3002 Black TPU, 50% Long Glass Reinforced
 43Toyobo Celstran® TPU-GF50-01 AF3001 Natural TPU, 50% Long Glass Reinforced
 44Toyobo Celstran® TPU-GF60-01 AF3001 Natural TPU, 60% Long Glass Reinforced
 45LATI Lastane 50 G/25 PUR, 25% Glass Fiber Reinforced
 46DiscontinuedLATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
 47MTI ThermoStran® TPU-40G Long Glass Fiber Compound
 48MTI ThermoStran® TPU-50G Long Glass Fiber Compound
 49MTI ThermoStran® TPU-60G Long Glass Fiber Compound
 50Nevicolor NEVITECH TPU G30 NATURALE Polyurethane, 30% Glass Fiber Reinforced
 
Found 105 Results -- Page of 3 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Instructions: This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database.  Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the 'Find' button next to its box.  You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.


Proto3000 - Rapid Prototyping

Notes:

Top

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.