MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Material Category Search

Find a Material Category:
Select a Material Category: Selected Material Category:
  Search Results
There are 41 materials in the category Polyvinyl Dichloride (PVDC). If your material is not listed, please refer to our search strategy page for assistance in limiting your search.

Found 41 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Polyvinyl Dichloride (PVDC)
 2DiscontinuedSK Chemicals Saran® 313 PVDC
 3DiscontinuedSK Chemicals Saran® 416 PVDC
 4DiscontinuedSK Chemicals Saran® 469 PVDC
 5DiscontinuedSK Chemicals Saran® 510 PVDC
 6DiscontinuedSK Chemicals Saran® 516 PVDC
 7DiscontinuedSK Chemicals Saran® 525 PVDC
 8DiscontinuedSK Chemicals Saran® 867 PVDC
 9DiscontinuedSK Chemicals Saran® F-239 PVDC
 10DiscontinuedSK Chemicals Saran® F-279 PVDC
 11DiscontinuedSK Chemicals Saran® F-310 PVDC
 12DiscontinuedSK Chemicals Saran® MA 119 PVDC
 13Syensqo (Solvay Specialty Polymers) Diofan® 193 D PVDC
 14Syensqo (Solvay Specialty Polymers) Diofan® A 050 PVDC
 15Syensqo (Solvay Specialty Polymers) Diofan® A 063 PVDC
 16Syensqo (Solvay Specialty Polymers) Diofan® A 297 PVDC
 17Syensqo (Solvay Specialty Polymers) Diofan® A 299 PVDC
 18Syensqo (Solvay Specialty Polymers) Diofan® A 586 PVDC
 19Syensqo (Solvay Specialty Polymers) Diofan® A 602 PVDC
 20Syensqo (Solvay Specialty Polymers) Diofan® A 610 PVDC
 21Syensqo (Solvay Specialty Polymers) Diofan® A 736 PVDC
 22Syensqo (Solvay Specialty Polymers) Diofan® B 203 PVDC
 23Syensqo (Solvay Specialty Polymers) Diofan® B 204 PVDC
 24Syensqo (Solvay Specialty Polymers) Diofan® B 206 PVDC
 25Syensqo (Solvay Specialty Polymers) Diofan® P 520 PVDC
 26Syensqo (Solvay Specialty Polymers) Diofan® P 530 PVDC
 27Syensqo (Solvay Specialty Polymers) Ixan® PVS 109 PVDC
 28Syensqo (Solvay Specialty Polymers) Ixan® PVS 119 PVDC
 29Syensqo (Solvay Specialty Polymers) Ixan® PVS 125 PVDC
 30Syensqo (Solvay Specialty Polymers) Ixan® PVS 801 PVDC
 31Syensqo (Solvay Specialty Polymers) Ixan® PVS 802 PVDC
 32Syensqo (Solvay Specialty Polymers) Ixan® PVS 827 PVDC
 33Syensqo (Solvay Specialty Polymers) Ixan® PVS 855 PVDC
 34Syensqo (Solvay Specialty Polymers) Ixan® PVS 856 PVDC
 35Syensqo (Solvay Specialty Polymers) Ixan® SGA-1 PVDC
 36DiscontinuedSyensqo (Solvay Specialty Polymers) Ixan® PVS 706 Polyvinylidene Chloride (PVDC)
 37DiscontinuedSyensqo (Solvay Specialty Polymers) Diofan® A 036 Polyvinylidene Chloride (PVDC)
 38DiscontinuedSyensqo (Solvay Specialty Polymers) Diofan® A602 Polyvinylidene Chloride (PVDC)
 39DiscontinuedSyensqo (Solvay Specialty Polymers) Diofan® A610 Polyvinylidene Chloride (PVDC)
 40DiscontinuedSyensqo (Solvay Specialty Polymers) Diofan® P510 Polyvinylidene Chloride (PVDC)
 41DiscontinuedSyensqo (Solvay Specialty Polymers) Diofan® P530 Polyvinylidene Chloride (PVDC)
 
Found 41 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Instructions: This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database.  Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the 'Find' button next to its box.  You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.


Proto3000 - Rapid Prototyping

Notes:

Top

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.