System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Material Category Search
User Input Problem
Find a Material Category:
Select a Material Category:
Carbon (866 matls)
Ceramic (10004 matls)
Fluid (7562 matls)
Metal (17052 matls)
Other Engineering Material (8063 matls)
Polymer (97635 matls)
Pure Element (507 matls)
Wood and Natural Products (398 matls)
Selected Material Category:
Search Results
There are
335
materials in the category
AISI 8000 Series Steel
. If your material is not listed, please refer to our
search strategy
page for assistance in limiting your search.
Found
335
Results
-- Page
1
2
3
4
5
6
7
of
7
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Use Folder
Contains
New Folder Name
My Folder
Select
Material Name
1
Overview of materials for AISI 8000 Series Steel
2
AISI 8115 Low Alloy Steel, Cold Drawn Bar
3
AISI 81B45 Steel
4
AISI 81B45H Steel
5
AISI 8615 Steel, heat treated, 150°C (300°F) temper, 25 mm bar
6
AISI 8617 Steel, heat treated, machined, pseudocarburized, 150°C (300°F) temper
7
AISI 8617 Steel, heat treated, machined, pseudocarburized, reheated to 855°C (1570°F), 150°C (300°F) temper
8
AISI 8617 Steel, heat treated, machined, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper
9
AISI 8617 Steel, double quenched, 150°C (300°F) temper
10
AISI 8617H Steel, heat treated, machined, pseudocarburized, 150°C (300°F) temper
11
AISI 8617H Steel, heat treated, machined, pseudocarburized, reheated to 855°C (1570°F), 150°C (300°F) temper
12
AISI 8617H Steel, heat treated, machined, pseudocarburized, reheated to 800°C (1470°F), 150°C (300°F) temper
13
AISI 8617H Steel, double quenched, 150°C (300°F) temper
14
AISI 8620 Steel, annealed 13 mm (0.5 in.) round
15
AISI 8620 Steel, normalized, 13 mm (0.5 in.) round
16
AISI 8620 Steel, quenched from carburizing box, 13 mm (0.5 in.) round
17
AISI 8620 Steel, quenched from carburizing box, 25 mm (1 in.) round
18
AISI 8620 Steel, quenched from carburizing box, 50 mm (2 in.) round
19
AISI 8620 Steel, cooled in carburizing box, reheated and quenched, 13 mm (0.5 in.) round
20
AISI 8620 Steel, carburized, box cooled, reheated and quenched, 150°C (300°F) temper, 25 mm (1 in.) round
21
AISI 8620 Steel, carburized, box cooled, reheated and quenched, 150°C (300°F) temper, 50 mm (2 in.) round
22
AISI 8620 Steel, carburized, box cooled, reheated and double quenched, 150°C (300°F) temper, 13 mm (0.5 in.) round
23
AISI 8620 Steel, quenched from 900°C (1650°F),tempered at 150°C (300°F), Low temp impact properties
24
AISI 8620 Steel, quenched from 900°C (1650°F), tempered at 425°C (800°F), Low temp impact properties
25
AISI 8620 Steel, quenched from 900°C (1650°F), tempered at 540°C (1000°F), Low temp impact properties
26
AISI 8620 Steel, quenched from 900°C (1650°F), tempered at 650°C (1200°F), Low temp impact properties
27
AISI 8620 Steel, direct quenched from pot, 150°C (300°F) temper, carburized
28
AISI 8620 Steel, single quenched and tempered (150°C (300°F)), carburized
29
AISI 8620 Steel, double quenched and tempered (150°C (300°F)), carburized
30
AISI 8620 Steel, direct quenched from pot, 230°C (450°F) temper, carburized
31
AISI 8620 Steel, single quenched and tempered (230°C (450°F)), carburized
32
AISI 8620 Steel, double quenched and tempered (230°C (450°F)), carburized
33
AISI 8620 Steel, normalized, machined to 25 mm, pseudocarburized, reheated to 775°C, 150°C temper
34
AISI 8620 Steel, normalized, machined to 25 mm, pseudocarburized, reheated to 800°C, 150°C temper
35
AISI 8620 Steel, normalized, machined to 25 mm, pseudocarburized, reheated to 845°C, 150°C temper
36
AISI 8620 Steel, normalized, machined to 25 mm, pseudocarburized, oil quenched, 150°C temper
37
AISI 8620 Steel, normalized, machined to 13.7 mm, pseudocarburized, reheated to 775°C, 150°C temper
38
AISI 8620 Steel, normalized, machined to 13.7 mm, pseudocarburized, reheated to 800°C, 150°C temper
39
AISI 8620 Steel, normalized, machined to 13.7 mm, pseudocarburized, reheated to 840°C, 150°C temper
40
AISI 8620 Steel, normalized, machined to 13.7 mm, pseudocarburized, oil quenched, 150°C temper
41
AISI 8620 Steel, annealed 25 mm (1 in.) round
42
AISI 8620 Steel, normalized (heated to 915°C air cooled), 13 mm (0.5 in.) round
43
AISI 8620 Steel, normalized, 25 mm (1 in.) round
44
AISI 8620 Steel, normalized, 50 mm (2 in.) round
45
AISI 8620 Steel, normalized, 100 mm (4 in.) round
46
AISI 8620 Steel, mock carburized, reheated and oil quenched, 150°C (300°F) temper, 13 mm (0.5 in.) round
47
AISI 8620 Steel, mock carburized, reheated and oil quenched, 150°C (300°F) temper, 25 mm (1 in.) round
48
AISI 8620 Steel, mock carburized, reheated and quenched, 150°C (300°F) temper, 50 mm (2 in.) round
49
AISI 8620 Steel, mock carburized, reheated and oil quenched, 150°C (300°F) temper, 100 mm (4 in.) round
50
AISI 8620 Steel, mock carburized, reheated and oil quenched, 230°C (450°F) temper, 13 mm (0.5 in.) round
Found
335
Results
-- Page
1
2
3
4
5
6
7
of
7
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Instructions:
This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database. Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the
'Find'
button next to its box. You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.
Proto3000 - Rapid Prototyping
Notes:
Visit MatWeb's
property-based search page
to limit your results to materials that meet specific property performance criteria.
Text searches can be done from any page - use the
Quick Search
box in the top right of the page.
More
Search Strategies
on how to find information in MatWeb.
Show All Materials
- an inefficient drill-down to data sheets. Registered users who are logged in omit a step in this drill down process.
Top
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.