MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Material Category Search

Find a Material Category:
Select a Material Category: Selected Material Category:
  Search Results
There are 131 materials in the category Acetal Copolymer, PTFE Filled. If your material is not listed, please refer to our search strategy page for assistance in limiting your search.

Found 131 Results -- Page of 3 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Acetal Copolymer, PTFE Filled
 2Mocom (ALBIS) ALCOM® POM 770/1 PTFE10 POM, 10% PTFE Reinforced
 3Mocom (ALBIS) ALCOM® POM 770/1 PTFE15 POM, 15% PTFE Reinforced
 4Mocom (ALBIS) ALCOM® POM 770/1 PTFE18 SI2 POM, 20% PTFE/Silicone
 5Mocom (ALBIS) ALCOM® POM 770/1 PTFE20 POM, 20% PTFE
 6Mocom (ALBIS) ALCOM® WP POM 5020 TF 18029 POM, 20% PTFE/Aramid Reinforced
 7Mocom (ALBIS) ALCOM® POM 770/1 PTFE1,5 POM, 1.5% PTFE Reinforced
 8Bada BADAFORM® C110 TF20 natural POM, 20% PTFE Filled
 9CENTROPLAST CENTRODAL TF Polyoxymethylene + PTFE
 10DiscontinuedClariant Renol POMSP0001 Acetal Copolymer, Aramid Fiber, PTFE Lubricated
 11Colour Image Plastic Compound Smoothblend® POM-1200 POM, 10% PTFE Filled
 12Colour Image Plastic Compound Smoothblend® POM-1400 POM, 20% PTFE Filled
 13Delrin Delrin® 100AF POM-PTFE20
 14Delrin Delrin® 100TL NC010 POM-SD
 15Delrin Delrin® 500AF POM-SF20
 16Delrin Delrin® 500TL NC010 POM-SD
 17Delrin Delrin® 520MP NC010 POM-SD20
 18Ensinger TECACOMP POM TRM natural 1064527 POM-C, Silicone Oil/PTFE Filled
 19Eurotec® Tecoform® PO20 NL RT POM, PTFE modified, natural
 20Celanese Celcon® CFX-0308 PTFE and Silicone Modified Acetal Copolymer
 21Celanese Celcon® LW90F5 Tetrafluoroethylene Filled Acetal Copolymer
 22Celanese Celcon® MT24F02 Acetal Copolymer
 23Celanese Celcon® MT24F01 Medical Grade Acetal Copolymer
 24DiscontinuedAvient Lubri-Tech™ AT-000/02T Acetal - 2% PTFE
 25DiscontinuedAvient Lubri-Tech™ AT-000/08T Acetal - 8% PTFE
 26DiscontinuedAvient Lubri-Tech™ AT-000/15T-2S Copolymer Acetal - 15% PTFE, 2% Silicone Lubricated
 27DiscontinuedAvient Lubri-Tech™ AT-15GP/05T Acetal With Graphite - 5% PTFE
 28KEP Kepital® FL2005 Acetal Copolymer, PTFE Filled
 29KEP Kepital® FL2010 Acetal Copolymer, PTFE modified
 30KEP Kepital® FL2020 Acetal Copolymer, PTFE modified
 31Kolon KOCETAL® TF302 Wear Modified Acetal Resin
 32Kolon KOCETAL® TF304 Wear Modified Acetal Resin
 33LATI Latilub 73/13-10ST POM, Silicone/PTFE Filled
 34LATI Latilub 73/13-10T Y/15 POM, 15% Aramid Fiber Reinforced, PTFE Filled
 35LATI Latilub 73/13-20T POM, PTFE Filled
 36Cheng Yu Plastic SW10 POM/PTFE
 37Cheng Yu Plastic SW15 POM/PTFE
 38Cheng Yu Plastic SW02 POM/PTFE
 39Lehvoss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer with PTFE, lubricant modified
 40DiscontinuedLehvoss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer with PTFE
 41Lehvoss LUVOCOM® 80-7014 Polyacetal-copolymer with PTFE
 42Lehvoss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer with PTFE
 43Manifattura Cattaneo POM c+PTFE Acetal, PTFE Filled
 44Mitsubishi Iupital® FL2010 Copolymer Acetal
 45Mitsubishi Iupital® FL2020 Copolymer Acetal
 46Orion Performance Compounds i-OnLube™ POM L05 Provisional Data, Acetal Copolymer, 5% PTFE Filled
 47Orion Performance Compounds i-OnLube™ POM L22 Acetal Copolymer, 20% PTFE Filled/2% Silicone Lubricated
 48Petropol Tenopom® B3 P15 PRTA010 PR331 POM, PTFE Filled
 49Petropol Tenopom® B3 P15 S2 NTLA016 PR341 POM, PTFE Filled, Dry
 50Petropol Tenopom® B3 P15 S2 NTLA016 PR341 POM, PTFE Filled, Conditioned
 
Found 131 Results -- Page of 3 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Instructions: This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database.  Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the 'Find' button next to its box.  You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.


Proto3000 - Rapid Prototyping

Notes:

Top

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.