MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Material Category Search

Find a Material Category:
Select a Material Category: Selected Material Category:
  Search Results
There are 32 materials in the category Nylon 612, Carbon Fiber Filler. If your material is not listed, please refer to our search strategy page for assistance in limiting your search.

Found 32 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page
Use Folder Contains  
Select Material Name
 1Overview of materials for Nylon 612, Carbon Fiber Filler
 2A. Schulman ComAlloy Lubrilon® 646 Nylon 6/12, Carbon Fiber/PTFE Reinforced
 3Bada BADAMID® PA612 CF10 TM-Z2 black S1 PA612, 10% Carbon Fiber Reinforced, Dry
 4Bada BADAMID® PA612 CF10 TM-Z2 black S1 PA612, 10% Carbon Fiber Reinforced, Conditioned
 5Evonik VESTAMID® DX9180 BK Nylon 612, Carbon Fiber Reinforced
 6Evonik VESTAMID® L-CF15 BK E70461 Nylon 12, Carbon Fiber Reinforced
 7Polymaker PolyMide™ PA12-CF 3D Printing Filament
 8RTP Company RTP 285 D TFE 15 A Nylon 6/12 (PA), Carbon Fiber - PTFE Lubricated
 9RTP Company RTP 283 D TFE 10 SI 2 Nylon 6/12 (PA); Carbon Fiber - PTFE Lubricated - Silicone Lubricated
 10RTP Company RTP 285 D TFE 15 Nylon 6/12 (PA) Carbon Fiber - PTFE Lubricated
 11RTP Company RTP 285 D TFE 13 SI 2 Nylon 6/12 (PA) Carbon Fiber - PTFE Lubricated - Silicone Lubricated
 12RTP Company RTP 281 D TFE 10 Nylon 6/12 (PA), Carbon Fiber - PTFE Lubricated
 13RTP Company RTP 283 D TFE 15 Nylon 6/12 (PA), Carbon Fiber - PTFE Lubricated
 14RTP Company RTP 283 D TFE 15 SI 2 Nylon 6/12 (PA), Carbon Fiber - PTFE Lubricated - Silicone Lubricated
 15RTP Company RTP 285 D SI 2 Nylon 6/12 (PA), Carbon Fiber - Silicone Lubricated
 16RTP Company RTP 287 D Nylon 6/12 (PA), Carbon Fiber
 17RTP Company RTP 285 D Nylon 6/12 (PA), Carbon Fiber
 18RTP Company RTP 282 D TFE 15 Nylon 6/12 (PA), Carbon Fiber - PTFE Lubricated - Preliminary Data
 19DiscontinuedRTP Company RTP 280.8D  Nylon 6/12 (PA 6/12) Carbon Fiber 8%
 20DiscontinuedRTP Company RTP 281D  Nylon 6/12 (PA 6/12) Carbon Fiber 10%
 21DiscontinuedRTP Company RTP 281.3D  Nylon 6/12 (PA 6/12) Carbon Fiber 13%
 22DiscontinuedRTP Company RTP 286D FR  Nylon 6/12 (PA 6/12) Carbon Fiber 35% - Flame Retardant
 23DiscontinuedRTP Company RTP 285D TFE 10  Nylon 6/12 (PA 6/12) Carbon Fiber 30% - PTFE 10%
 24DiscontinuedRTP Company RTP 281D TFE 15  Nylon 6/12 (PA 6/12) Carbon Fiber 10% - PTFE 15%
 25DiscontinuedRTP Company RTP 285D TFE 15  Nylon 6/12 (PA 6/12) Carbon Fiber 30% - PTFE 15%
 26DiscontinuedRTP Company RTP 281D TFE 15 FR  Nylon 6/12 (PA 6/12) Carbon Fiber 10% - PTFE 15% - Flame Retardant
 27DiscontinuedRTP Company RTP 285D TFE 13 SI 2  Nylon 6/12 (PA 6/12) Carbon Fiber 30% - PTFE 13% - Silicone 2%
 28DiscontinuedRTP Company RTP 285D TFE 15 SI 2  Nylon 6/12 (PA 6/12) Carbon Fiber 30% - PTFE 15% - Silicone 2%
 29Techmer ES Electrafil® J-4/25/CF/15 BK PA6/12
 30Techmer ES Electrafil® J-4/25/CF/15 NAT PA6/12
 31Techmer ES HiFill® PA6/12 CF30 BK 30% Carbon Filled
 32Xenia Materials XECARB® 22-C30-ST PA6.12, 30% Carbon Fiber Reinforced
 
Found 32 Results -- Page of 1 -- [Prev Page] [Next Page] --  view per page

Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Instructions: This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database.  Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the 'Find' button next to its box.  You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.


Proto3000 - Rapid Prototyping

Notes:

Top

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.