System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Material Category Search
User Input Problem
Find a Material Category:
Select a Material Category:
Carbon (866 matls)
Ceramic (10004 matls)
Fluid (7562 matls)
Metal (17052 matls)
Other Engineering Material (8063 matls)
Polymer (97635 matls)
Pure Element (507 matls)
Wood and Natural Products (398 matls)
Selected Material Category:
Search Results
There are
55
materials in the category
PBT + ASA Blend, Glass Fiber Reinforced
. If your material is not listed, please refer to our
search strategy
page for assistance in limiting your search.
Found
55
Results
-- Page
1
2
of
2
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Use Folder
Contains
New Folder Name
My Folder
Select
Material Name
1
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
2
Akro-Plastic Precite® V GF 20 black (7736) PBT-ASA-GF 20
3
Akro-Plastic Precite® V GF 30 black (7723) PBT-ASA-GF 30
4
Mocom (ALBIS) ALTECH® PBT+ASA A 4212/507 MR/GF12 PBT+ASA 12% Glass Fiber/Mineral Reinforced
5
Mocom (ALBIS) ALTECH® PBT+ASA A 2020/510 GF20 PBT+ASA, 20% Glass Fiber Reinforced
6
Mocom (ALBIS) ALTECH® PBT+ASA A 4212/500 GF MR PBT+ASA, 12% Glass/Mineral Fiber Reinforced
7
Mocom (ALBIS) ALTECH® PBT+ASA A 4212/506 GF3M9 PBT+ASA, 12% Glass/Mineral Fiber Reinforced
8
Aurora Kunststoffe AUROdur® PBT+ASA GF20 black PBT/ASA Blend, 20% Glass Fiber Reinforced
9
Aurora Kunststoffe AUROdur® PBT+ASA GF30 black PBT/ASA Blend, 30% Glass Fiber Reinforced
10
Bada BADADUR® PBT/ASA 39 GF10 UV natural PBT/ASA, 10% Glass Fiber Reinforced
11
Barlog Plastics KEBALLOY ECO FE 221202 PBT/ASA, 20% Glass Fiber Reinforced
12
BASF Ultradur® S 4090 G4 BK15051 PBT/ASA, 20% Glass Reinforced
13
BASF Ultradur® S 4090 G2 10% Glass Filled PBT + ASA
14
BASF Ultradur® S 4090 GX 14% Glass Filled PBT + ASA
15
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT + ASA
16
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT + ASA
17
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT + ASA
18
Celanese Crastin® LW9020 BK580 PBT+ASA-GF20
19
Celanese Crastin® LW9020 NC010 PBT+ASA-GF20
20
Celanese Crastin® LW9020FR BK851 PBT+ASA-GF20FR(17)
21
Celanese Crastin® LW9020SF NC010 PBT + ASA-GF20
22
Celanese Crastin® LW9030 BK851 PBT+ASA-GF30
23
Celanese Crastin® LW9030 NC010 PBT+ASA-GF30
24
Celanese Crastin® LW9030FR BK851 PBT+ASA-GF30FR(17)
25
Celanese Crastin® LW9030FR NC010 PBT+ASA-GF30FR(17)
26
Eurotec® Tecodur® PB70 GR30 NL MB04 PBT/ASA, 30% glass fiber reinforced, heat & UV stabilized, natural
27
Kumho-Sunny HBA5810M PBT/ASA
28
Kumho-Sunny HBA5810G PBT/ASA, 10% Glass Fiber Reinforced
29
Kumho-Sunny HBA5820G PBT/ASA, 20% Glass Fiber Reinforced
30
Kumho-Sunny HBA5830G PBT/ASA, 30% Glass Fiber Reinforced
31
Envalior Pocan® A 3121 000000 PBT+ASA, 20% Glass Fiber Reinforced
32
Envalior Pocan® A 3131 000000 PBT+PC, 30% Glass Fiber Reinforced
33
Envalior Pocan® KU 1-7635 POS151 000000 PBT+PC, 30% Glass Fiber Reinforced
34
Envalior Pocan® C 3230 XF 000000 PBT+PC, 30% Glass Fiber Reinforced
35
Envalior Pocan® AF 4120 000000 PBT+ASA, 20% Glass Fiber Reinforced
36
Envalior Pocan® TP 740-101 000000 PBT+ASA, 15% Glass Fiber Filled
37
Envalior Pocan® A 3122 901510 PBT+ASA, 20% Glass Fiber
38
Envalior Pocan® A 3121 901510 PBT+ASA, 20% Glass Fiber
39
Envalior Pocan® TP 740-202 901510 PBT+ASA, 20% Glass Fiber
40
Lanxess Pocan® TP 740-201 000000 PBT + ASA, 20% Glass Fiber
41
LG Chemical LUMAX EU5300 PBT+ASA+GF30%, Injection Molding
42
Almaak Anjacom® PBT/ASA 465-GF15 PBT/ASA, 15% Glass Fiber Reinforced
43
Almaak Anjacom® PBT/ASA 468-GF15 PBT/ASA, 15% Glass Fiber Reinforced
44
Almaak Anjacom® PBT/ASA 465-GF30 PBT/ASA, 30% Glass Fiber Reinforced
45
Omni Plastics OmniTech™ PBSA GR30 PBT/ASA, 30% Glass Reinforced
46
Polykemi AB SCANBLEND P AP2060 F20 PBT/ASA, Glass Fiber Reinforced
47
Polykemi AB SCANBLEND P AP2060 F30 PBT/ASA, Glass Fiber Reinforced
48
Polykemi AB SCANBLEND FS7 F20 PBT/ASA Blend, Glass Fiber-Reinforced
49
Polyram RamLloy PFS302G14 ASA/PBT Alloy, 14% Glass Fiber
50
Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber
Found
55
Results
-- Page
1
2
of
2
--
[Prev Page]
[Next Page]
-- view
25
50
75
100
150
200
per page
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Instructions:
This page allows you to quickly access all of the polymers/plastics, metals, ceramics, fluids, and other engineering materials in the MatWeb material property database. Just select the material category you would like to find from the tree. Click on the [+] icon to open subcategory branches in the tree. Then click the
'Find'
button next to its box. You can then follow the links to the most complete data sheets on the Web, with information on over 1000 available properties, including dielectric constant, Poisson's ratio, glass transition temperature, dissipation factor, and Vicat softening point.
Proto3000 - Rapid Prototyping
Notes:
Visit MatWeb's
property-based search page
to limit your results to materials that meet specific property performance criteria.
Text searches can be done from any page - use the
Quick Search
box in the top right of the page.
More
Search Strategies
on how to find information in MatWeb.
Show All Materials
- an inefficient drill-down to data sheets. Registered users who are logged in omit a step in this drill down process.
Top
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.