MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sciengy PPS-SGL601E65 PPS, 60% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 60% Glass Fiber Filler

Material Notes: PPS-SGL601E65 PPS is a 60% special glass fiber and mineral reinforced low chlorine polyphenylene sulfide compound, its CL content is in 900PPM below, mainly used in the field of halogen content requirements.

Information provided by Shandong Sciengy New Materials Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³ISO 1183
Water Absorption at Saturation 0.020 %0.020 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inGB/T 15585
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inGB/T 15585
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 155 MPa22500 psiISO 527-2/1A
Elongation at Break 1.5 %1.5 %ISO 527-2/1A
Flexural Strength 240 MPa34800 psiISO 178
Flexural Modulus 19.5 GPa2830 ksiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmIEC 60093
Dielectric Constant 4.04.0IEC 60250
Dielectric Strength 16.0 kV/mm406 kV/inIEC 60243
Dissipation Factor 0.00200.0020IEC 60250
Comparative Tracking Index 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 260 °C500 °FISO 75-1/-2
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 330 °C554 - 626 °FInjection molding; ISO 294
Mold Temperature 120 - 160 °C248 - 320 °FInjection molding; ISO 294
Drying Temperature 150 °C
@Time 10800 sec
302 °F
@Time 3.00 hour
Injection Pressure 30.0 - 100 MPa4350 - 14500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCIE056 / 297103

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.