MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Strontium Neodymium Sulfide, SrNd2S4
Categories: Ceramic; Sulfide/Chalcogenide

Key Words: SrNd2S4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.18 g/cc0.187 lb/in³Theoretical
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 455 - 649455 - 649Alternate tests.
 590 - 630590 - 630Alternate tests.
 
Electrical PropertiesMetricEnglishComments
Band Gap 2.58 eV2.58 eVEstimated from absorption edge.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.3 µm/m-°C
@Temperature 20.0 - 100 °C
9.06 µin/in-°F
@Temperature 68.0 - 212 °F
Melting Point 1795 - 1855 °C3263 - 3371 °FFirst detectable sign of melting.
Solidus 1825 °C3317 °F
 
Descriptive Properties
ColorLight Green
Crystal StructureCubicTh3P4; I(-4)3d

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Platinum (II) Sulfide, PtS (Cooperite)
Platinum (II) Sulfide, PtS (Bragite)
Phosphorus (V) Sulfide Trichloride, PSCl3
Mateck GaAs
Mateck CdTe

BSUL03 / 294

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.