MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TRW VI A Cast Nickel Superalloy
Categories: Metal; Superalloy; Nickel Base

Material Notes: Typical Application: Turbine blade alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  82.7 MPa
@Temperature 1090 °C,
Time 360000 sec
12000 psi
@Temperature 2000 °F,
Time 100 hour
 131 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
19000 psi
@Temperature 1800 °F,
Time 1000 hour
 200 MPa
@Temperature 982 °C,
Time 360000 sec
29000 psi
@Temperature 1800 °F,
Time 100 hour
 421 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
61000 psi
@Temperature 1500 °F,
Time 1000 hour
 552 MPa
@Temperature 816 °C,
Time 360000 sec
80000 psi
@Temperature 1500 °F,
Time 100 hour
 896 MPa
@Temperature 649 °C,
Time 3.60e+6 sec
130000 psi
@Temperature 1200 °F,
Time 1000 hour
 1000 MPa
@Temperature 649 °C,
Time 360000 sec
145000 psi
@Temperature 1200 °F,
Time 100 hour
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.4 %5.4 %
Boron, B 0.020 %0.020 %
Carbon, C 0.13 %0.13 %
Chromium, Cr 6.0 %6.0 %
Cobalt, Co 7.5 %7.5 %
Hafnium, Hf 0.13 %0.13 %
Nickel, Ni 63.89 %63.89 %As Balance
Niobium, Nb (Columbium, Cb) 0.50 %0.50 %
Rhenium, Re 0.50 %0.50 %
Tantalum, Ta 9.0 %9.0 %
Titanium, Ti 1.0 %1.0 %
Tungsten, W 5.8 %5.8 %
Zirconium, Zr 0.13 %0.13 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Weartech International WT-306 Cobalt Hardfacing & Wear Resistant Alloy
TIMET TIMETAL® 367 (Ti-6Al-7Nb) Implant Grade Titanium Alloy
Ti30Nb ß titanium alloy
Ti-25Al-10Nb-3V-1Mo Titanium Aluminide
Ti-24Al-14Nb Titanium Aluminide

NZ97043 / 191442

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.