MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company EMI 2562 Polycarbonate/ABS Alloy (PC/ABS), Stainless Steel Fiber - Electrically Conductive - EMI/RFI Shielding
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Antistat/Conductive; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.32 g/cc1.32 g/ccASTM D 792
Additive Loading 15 %15 %Primary Additive
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0060 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 62.7 MPa9100 psiASTM D 638
Elongation at Break 3.0 - 5.0 %3.0 - 5.0 %ASTM D 638
Tensile Modulus 3.31 GPa480 ksiASTM D 638
Flexural Strength 112 MPa16200 psiASTM D 790
Flexural Modulus 3.52 GPa510 ksiASTM D 790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.20 mm
1.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.0 ohm-cm<= 1.0 ohm-cmASTM D 257
Surface Resistance <= 1000 ohm<= 1000 ohmESD STM11.11
Surface Resistivity per Square <= 10000 ohm<= 10000 ohmASTM D 257; ESD STM11.11
Static Decay <= 0.50 sec<= 0.50 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
Shielding Effectiveness  85 dB
@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
85 dB
@Thickness 0.118 in,
Frequency 3.00e+7 Hz
ASTM D 4935
 89 dB
@Thickness 3.00 mm,
Frequency 1.50e+8 Hz
89 dB
@Thickness 0.118 in,
Frequency 1.50e+8 Hz
ASTM D 4935
 92 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
92 dB
@Thickness 0.118 in,
Frequency 3.00e+8 Hz
ASTM D 4935
 98 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
98 dB
@Thickness 0.118 in,
Frequency 5.00e+8 Hz
ASTM D 4935
 103 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
103 dB
@Thickness 0.118 in,
Frequency 7.00e+8 Hz
ASTM D 4935
 105 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
105 dB
@Thickness 0.118 in,
Frequency 1e+9 Hz
ASTM D 4935
 106 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
106 dB
@Thickness 0.118 in,
Frequency 1.30e+9 Hz
ASTM D 4935
 106 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
106 dB
@Thickness 0.118 in,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D 648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 243 - 274 °C470 - 525 °F
Mold Temperature 51.7 - 93.3 °C125 - 200 °F
Drying Temperature 93.3 °C
@Time 14400 sec
200 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company EMI 2185  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 30%
RTP Company EMI 2184  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 25%
RTP Company EMI 2183  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 20%
RTP Company EMI 2162 Polyetherimide (PEI); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection
RTP Company EMI 1382  Polyphenylene Sulfide (PPS) Shielding - Nickel-Coated Carbon Fiber 15%

PQZWA3866 / 91783

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.