MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gabriel Fluorolube® T-80 CTFE Fluoropolymer Oil
Categories: Fluid; Lubricant; Fluoropolymer Base

Material Notes: Fluorolube® oil is a liquid lubricant that delivers long-lasting lubrication for metallic surfaces (except copper, aluminum and magnesium) in applications requiring stability and performance in strongly acidic and/or oxidizing environments. It is a saturated, hydrogen-free, low-molecular weight polymers of chlorotrifluoroethylene (CTFE) that combines high-temperature performance, non-flammability and chemical inertness under many demanding conditions. Available in a range of viscosities, Fluorolube® oils are compatible with chlorine, oxygen, hydrogen peroxide, red fuming nitric acid and other strong oxidizing agents, and are nonflammable.

Information provided by Gabriel Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.893 g/cc
@Temperature 71.0 °C
0.06839 lb/in³
@Temperature 160 °F
Typical
 1.945 g/cc
@Temperature 38.0 °C
0.07027 lb/in³
@Temperature 100 °F
Typical
pH 6.0 - 7.56.0 - 7.5pH of water extract; specification
Viscosity  <= 77 cP
@Temperature 71.0 °C
<= 77 cP
@Temperature 160 °F
Typical
 65 - 95 cP
@Temperature 71.0 °C
65 - 95 cP
@Temperature 160 °F
Specification
 <= 970 cP
@Temperature 38.0 °C
<= 970 cP
@Temperature 100 °F
Typical
Viscosity Measure  41 cSt
@Temperature 71.0 °C
41 cSt
@Temperature 160 °F
Typical
 500 cSt
@Temperature 38.0 °C
500 cSt
@Temperature 100 °F
Typical
 
Thermal PropertiesMetricEnglishComments
CTE, linear 509 µm/m-°C283 µin/in-°FDensity Correction Factor = 8.5 x 10-4/°F
Maximum Service Temperature, Air 150 - 315 °C302 - 599 °Fdepends on time and environment
Pour Point 3.00 - 5.00 °C37.4 - 41.0 °F
 
Descriptive Properties
CAS Number9002-83-9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

VGABR893 / 230700

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.