MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celcon® GC20 POM, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 20% Glass Fiber Reinforced

Material Notes: Celcon« GC20 is a glass coupled formulation containing 20% fiber glass reinforcement to improve strength and stiffness.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 99.0 MPa14400 psi5mm/min; ISO 527-2/1A
Elongation at Break 2.2 %2.2 %5mm/min; ISO 527-2/1A
Tensile Modulus 7.30 GPa1060 ksi50mm/min; ISO 527-2/1A
Flexural Strength 130 MPa18900 psiISO 178
Flexural Modulus 7.00 GPa1020 ksiISO 178
Izod Impact, Notched (ISO) 5.20 kJ/m²2.47 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 43.0 µm/m-°C23.9 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
Melting Point 165 °C329 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 90.0 - 120 °C194 - 248 °Fcavity
 190 - 210 °C374 - 410 °Fhot runner
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 180 - 190 °C356 - 374 °F
Zone 4 190 - 200 °C374 - 392 °F
Die Temperature 190 - 200 °C374 - 392 °F
Melt Temperature 180 - 200 °C356 - 392 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 90.0 - 140 MPa13100 - 20300 psi
Hold Pressure 90.0 - 140 MPa13100 - 20300 psi
Back Pressure <= 2.00 MPa<= 290 psi
 
Descriptive Properties
Injection moldingYes
Injection speedslow
PelletsYes
Processing conditions acc. ISO9988-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 100 NC010 POM
Celanese Celcon® M90™ POM, Unfilled
Celanese Celcon® GC10 POM, 10% Glass Reinforced
Celanese Celcon® GC15 POM, 15% Glass Reinforced
Delrin Delrin® 111DP NC010 POM

PHCQ102 / 178557

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.