MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Einsteinium, Es
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Physical Form: Metal; Cubic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.84 g/cc0.319 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 252252Longest-Lived Isotope (1995)
Atomic Number 9999
X-ray Absorption Edge 0.09068 Å0.09068 ÅK
 0.46357 Å0.46357 ÅLI
 0.48009 Å0.48009 ÅLII
 0.60645 Å0.60645 ÅLIII
Electronegativity 1.31.3Pauling
 
Mechanical PropertiesMetricEnglishComments
Bulk Modulus 15.0 GPa2180 ksiEstimated
 
Thermal PropertiesMetricEnglishComments
Melting Point 860 °C1580 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 
Component Elements PropertiesMetricEnglishComments
Einsteinium, Es 100 %100 %
 
Descriptive Properties
CAS Number7429-92-7

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Erbium, Er
Darmstadtium, Ds
Dubnium, Db
Chromium, Cr; Recrystallized
Copper, Cu; Cold-Worked

AMEEs00 / 33

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.