MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chi Mei Kibisan® PN-107 L125 SAN
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: High Clarity

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Melt Flow 32 g/10 min
@Load 10.0 kg,
Temperature 220 °C
32 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Melt Volume Rate (ml/10 min); ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 155 MPa22500 psiH358/30; ISO 2039-1
Tensile Strength at Break 54.0 MPa7830 psi50 mm/min; ISO 527
Tensile Strength, Yield 52.0 MPa7540 psi50 mm/min; ISO 527
Elongation at Break 4.0 %4.0 %50 mm/min; ISO 527
Flexural Strength 92.0 MPa13300 psi2 mm/min; ISO 178
Flexural Modulus 3.00 GPa435 ksi2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180/1C
Charpy Impact Unnotched 1.80 J/cm²8.57 ft-lb/in²ISO 179
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179
Impact 3.03.0Impact Flexural Test Notched (KJ/m²)
 1818Impact Flexural Test Unnotched (KJ/m²)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °Funannealed; ISO 75
 97.0 °C207 °Fannealed; ISO 75
Vicat Softening Point  101 °C
@Load 5.00 kg
214 °F
@Load 11.0 lb
50°C/hr; ISO 306
 103 °C
@Load 5.00 kg
217 °F
@Load 11.0 lb
120°C/hr; ISO 306
 105 °C
@Load 1.00 kg
221 °F
@Load 2.20 lb
50°C/hr; ISO 306
 108 °C
@Load 1.00 kg
226 °F
@Load 2.20 lb
120°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
UL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Kibisan® PN-127 SAN
Chi Mei Kibisan® PN137H SAN Resin, General Purpose
Chi Mei Kibisan® PN-106 L150 SAN
Chi Mei Kibisan® PN-117 SAN
Chi Mei Kibisan® PN107 SAN Resin, General Purpose

PCHI974 / 109462

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.