MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zoltek™ PX30 PW06 (Plain Weave) Carbon Fiber Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX30 Woven Carbon Fabrics tailorability results from controlling the yield on rovings and yarns, and allows for a variety of finished composite thicknesses. The spun yarns have many surface fibrils that protrude in various directions at various lengths from the surface. This fiber loft contributes to high cross-ply tensile and interlaminar shear strengths for 2-D composite materials. Contour conformation without wrinkling is another advantage of spun yarn fabrics. ZOLTEK PX30 materials undergo high temperature carbonization process, involving a long temperature soak time, resulting in a very thermally stable and chemically pure fabric with low oxidation rate.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³
Thickness 673 microns26.5 milCured
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00140 ohm-cm0.00140 ohm-cm
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 99 %99 %
 
Descriptive Properties
Areal Weight237 g/m2
Oxidation Rate1% per hour @ 932°F
Roll Length36m
Roll Width1067 mm
Warp and Fill113x113 yarns/10cm
Yarn Input2/10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
Graphite, Carbon, C
Hexcel® HexTow® IM5 Intermediate Modulus Carbon Fiber (12,000 Filaments)
Hexcel® HexTow® IM6 Intermediate Modulus Carbon Fiber (12,000 Filaments)
Sinotek Materials Packing Carbon Fiber with Graphite

ECZO834 / 232309

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.