MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Commercial Rolled Zinc (Zn-0.08Pb), Cold-Rolled - Transverse Properties
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Hot Work Temperature 120-275°C

Properties vary with rolling direction. Average values and values for longitudinal direction are listed separately.

Key Words: UNS Z21210
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.14 g/cc0.258 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 186 MPa27000 psi
Elongation at Break 40 %40 %in 5 cm
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000620 ohm-cm0.00000620 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.4 µm/m-°C
@Temperature 20.0 °C
13.0 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.395 J/g-°C0.0944 BTU/lb-°F
Thermal Conductivity 108 W/m-K750 BTU-in/hr-ft²-°F
Melting Point 419 °C786 °F
Solidus 419 °C786 °FMelting Point
Liquidus 419 °C786 °FMelting Point
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 120 - 275 °C248 - 527 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0010 %<= 0.0010 %
Cadmium, Cd <= 0.0050 %<= 0.0050 %
Copper, Cu <= 0.0010 %<= 0.0010 %
Iron, Fe <= 0.012 %<= 0.012 %
Lead, Pb <= 0.10 %<= 0.10 %
Tin, Sn <= 0.0010 %<= 0.0010 %
Zinc, Zn >= 99.88 %>= 99.88 %As balance; per ASTM B 69

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Cold-Rolled
Commercial Rolled Zinc (Zn-0.08Pb), Hot-Rolled - Transverse Properties
Commercial Rolled Zinc (Zn-0.08Pb), Hot-Rolled - Longitudinal Properties
Commercial Rolled Zinc (Zn-0.08Pb), Hot-Rolled
Commercial Rolled Zinc (Zn-0.08Pb), Cold-Rolled - Longitudinal Properties

MZN723 / 14545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.