MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals Sclair® 2508-UV9 MDPE Injection Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded

Material Notes: Features: Excellent processability for applications requiring stiffness and toughness, good cold temperature impact properties.

Applications: Roll-out cart lids.

Data provided by the manufacturer.

Key Words: Medium Density Polyethylene
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.941 g/cc0.0340 lb/in³ASTM D792
ESCR 100% Igepal® 30 hour30 hourF50, Condition A, ASTM D1693
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength, Yield 19.0 MPa2760 psiASTM D638
Elongation at Break 400 %400 %ASTM D638
Flexural Modulus 0.600 GPa87.0 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 119 °C246 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 - 215 °C338 - 419 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 2272 Polyethylene, Injection Grade
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin
NOVA Chemicals Sclair® 2709 HDPE Injection Molding Resin
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin

PEHN1K / 35569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.