MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials HiDura™ PTR 75HB NT0679 Nylon PA66/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: HiDura PTR 75HB NT0679 is a high-viscosity, heat-stabilized polyamide copolymer resin designed for extrusion applications. This product is available in natural only. It offers a well-balanced combination of engineering properties characterized by high melt point, high strength and flexibly, toughness and good chemical resistance. Specifically, its reduced crystallization, high melt point and heat stabilization make it a great solution for films being used in cooking or autoclave curing applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³DAM; ISO 1183
Moisture Absorption <= 0.100 %<= 0.100 %ASTM D 6869
Moisture Absorption at Equilibrium 2.4 %2.4 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 11 %11 %ISO 62
Viscosity Measurement 4.14.1Relative Viscosity; Sulfuric Acid; ISO 307
 >= 165>= 165Relative Viscosity; Formic Acid; ASTM D 789
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 78.0 MPa11300 psiDAM; ISO 527-2
Elongation at Break 170 %170 %DAM; ISO 527-2
Flexural Strength 84.0 MPa12200 psiDAM; ISO 178
Charpy Impact, Notched 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 243 °C469 °FDAM; ISO 11357-3
 
Processing PropertiesMetricEnglishComments
Zone 1 275 - 290 °C527 - 554 °FExtrusion
Zone 2 275 - 290 °C527 - 554 °FExtrusion
Zone 3 270 - 285 °C518 - 545 °FExtrusion
Zone 4 260 - 275 °C500 - 527 °FExtrusion
Zone 5 255 - 270 °C491 - 518 °FExtrusion
Die Temperature 270 - 290 °C518 - 554 °FExtrusion
Melt Temperature 270 - 290 °C518 - 554 °FExtrusion
Drying Temperature 70.0 - 80.0 °C158 - 176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AppearanceNatural Color
FeaturesChemical Resistant
 Good Toughness
 High Melt Stability
 High Rigidity
 High Strength
 Medium-High Viscosity
FormsPellets
Processing MethodOther Extrusion
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8603 / 293352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.