MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ecovio® C2332 F Blend Biodegradable Polyester
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polylactic Acid (PLA) Biopolymer

Material Notes: Ecovio® F Blend C2332 is a biodegradable film product containing 18% renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic acid (PLA). Due to its outstanding mechanical strength Ecovio® F Film C2332 offers a great down gauging potential needed for thin film applications like garbage bags, organic waste bags, T-shirt bags, agricultural film etc. Ecovio® F Film C2332 already contains antiblocking and slip agents required for easy processing on film extrusion and film conversion equipment. Ecoflex® F Blend is the continuous phase in the structure of Ecovio® F Film C2332 transferring the beneficial film properties of Ecoflex® F Blend into the new product.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 135 g/m²/day8.69 g/100 in²/day
Oxygen Transmission Rate 1200 cc/m²/day77.3 cc/100 in²/daydry; ASTM D3985
Thickness 10.0 - 120 microns0.394 - 4.72 mil
 
Mechanical PropertiesMetricEnglishComments
Dart Drop Total Energy 240 J/cm0.450 ft-lb/milDIN 53373
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ecovio® C2203 F Blend Biodegradable Polyester
BASF Ecovio® C2224 F Blend Biodegradable Polyester
FKuR Kunststoff Bio-Flex® F 6514 PLA Blend
BASF Ecoflex® P BX 7020 Biodegradable Polyester
Overview of materials for Polylactic Acid (PLA) Biopolymer

PBASG0010 / 131644

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.