MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Radel® 5500 yellow Polyphenylsulfone
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes:
  • resistant to autoclaving
  • biocompatible
  • compliant with cytoxicity according to ISO 10993-5
  • meets requirements for USP Class VI
  • excellent impact strength
Target Industries:
  • medical technology
  • pharmaceutical industry
(TECASON® P MT)

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³
Moisture Absorption 1.10 %1.10 %saturation; ASTM D570
 0.370 %
@Time 86400 sec
0.370 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D 785
Tensile Strength, Yield 75.8 MPa11000 psiASTM D 638
Elongation at Yield 80 %80 %ASTM D 638
Modulus of Elasticity 2.41 GPa350 ksiASTM D 638
Flexural Strength 107 MPa15500 psiASTM D 790
Flexural Modulus 2.24 GPa325 ksiASTM D 790
Compressive Yield Strength 93.1 MPa
@Strain 10 %
13500 psi
@Strain 10 %
ASTM D 695
Compressive Strength 10.3 MPa
@Strain 1 %
1500 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 1.55 GPa225 ksiASTM D 695
Izod Impact, Unnotched 1.33 J/cm2.50 ft-lb/inASTM D 256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D 257
Dielectric Constant 3.44
@Frequency 60 Hz
3.44
@Frequency 60 Hz
50% RH; ASTM D 150
Dielectric Strength 14.2 kV/mm361 kV/inASTM D 149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.8 µm/m-°C31.0 µin/in-°FASTM D 696
Specific Heat Capacity 1.13 J/g-°C0.270 BTU/lb-°F
Maximum Service Temperature, Air 149 °C300 °FLong Term
 182 °C360 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 214 °C417 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 207 °C405 °FASTM D 648
Vicat Softening Point 218 °C424 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
Coloryellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8149 / 319077

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.