MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite Vyncolit® BXE650/1 Phenolic Novolac
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral Filled

Material Notes: Vyncolit® BXE650/1 is an inorganic filled phenolic molding compound with excellent isotropic properties, superior dimensional stability and very high mechanical properties, even at elevated temperatures.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Key Words: PF-(GB+GF)75
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.98 g/cc0.0715 lb/in³ISO 1183
Apparent Bulk Density 0.770 g/cc0.0278 lb/in³ISO 60
Water Absorption 0.050 %0.050 %ISO 62
Linear Mold Shrinkage 0.0019 cm/cm0.0019 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 108 MPa15700 psiISO 527-1
Elongation at Break 0.54 %0.54 %ISO 527-1
Tensile Modulus 22.0 GPa3190 ksiISO 527-1
Flexural Strength 235 MPa34100 psiISO 178
Flexural Modulus 20.0 GPa2900 ksiISO 178
Flexural Strain at Break 1.19 %1.19 %ISO 178
Compressive Strength 413 MPa59900 psiISO 604
Charpy Impact Unnotched 1.36 J/cm²6.47 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.290 J/cm²1.38 ft-lb/in²ISO 179-1
Coefficient of Friction, Dynamic 0.540.54
Coefficient of Friction, Static 0.560.56
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.10e+14 ohm-cm2.10e+14 ohm-cmIEC 60093
Surface Resistance 2.50e+12 ohm2.50e+12 ohmIEC 60093
Dielectric Strength 28.0 kV/mm711 kV/inIEC 60243-1
Comparative Tracking Index 225 V225 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 16.0 µm/m-°C8.89 µin/in-°FTMA
CTE, linear, Transverse to Flow 24.0 µm/m-°C13.3 µin/in-°FTMA
Thermal Conductivity 0.510 W/m-K3.54 BTU-in/hr-ft²-°FASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) >= 250 °C>= 482 °FISO 75 Af
Deflection Temperature at 8.0 MPa 178 °C352 °FISO 75 Cf
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage 0.040 %0.040 %Post; ISO 2577
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 2151T Thermally Conductive Electrically Insulating Compound
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade
Lord Adhesives CoolTherm™ EP-343 Thermally Conductive Epoxy Conformal Coating

PSUMIT493 / 194298

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.