MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Durafide® 6150T6 HF2000/HD9100 Linear Polyphenylene sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes: High impact.

Information provided by Polyplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.71 g/cc0.0618 lb/in³ISO 1183
Water Absorption 0.050 %
@Temperature 23.0 °C,
Time 86400 sec
0.050 %
@Temperature 73.4 °F,
Time 24.0 hour
1 mm thickness; ISO 62
Viscosity 240000 cP
@Frequency 100 Hz,
Temperature 310 °C
240000 cP
@Frequency 100 Hz,
Temperature 590 °F
Melt viscosity; ISO 11443
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9090ISO 2039-2
Tensile Strength 155 MPa22500 psiISO 527-1,2
Elongation at Break 1.7 %1.7 %ISO 527-1,2
Flexural Strength 225 MPa32600 psiISO 178
Flexural Modulus 13.2 GPa1910 ksiISO 178
Charpy Impact, Notched 0.950 J/cm²4.52 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+16 ohm-cm2.00e+16 ohm-cmIEC 60093
Dielectric Constant  4.4
@Frequency 1e+6 Hz
4.4
@Frequency 1e+6 Hz
IEC 60250
 4.5
@Frequency 1000 Hz
4.5
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm
@Thickness 3.00 mm
406 kV/in
@Thickness 0.118 in
IEC 60243-1
Dissipation Factor  0.0040
@Frequency 1000 Hz
0.0040
@Frequency 1000 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 126 sec126 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°F
CTE, linear, Transverse to Flow 40.0 µm/m-°C22.2 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FISO 75-1,2
Flammability, UL94 V-0V-0only black
 
Descriptive Properties
Yellow Card File No.E109088

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPL9899 / 305572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.