MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Calcium, Ca; Annealed
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Annealed applies only to tensile and/or hardness values; other property values are typical of the element.

MatWeb also has entries for Calcium, Rolled

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 40.07840.0781995
Atomic Number 2020
Thermal Neutron Cross Section 0.43 barns/atom0.43 barns/atom
X-ray Absorption Edge 3.07016 Å3.07016 ÅK
 31.068 Å31.068 ÅLI
 35.417 Å35.417 ÅLII
 35.827 Å35.827 ÅLIII
Electrode Potential -2.80 V-2.80 V
Electronegativity 1.01.0Pauling
Ionic Radius 0.990 Å0.990 ÅCrystal Ionic Radius for Valence +2
 1.18 Å1.18 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 0.747 g/A/h0.747 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1717
Tensile Strength, Ultimate 40.0 MPa5800 psi
Tensile Strength, Yield 13.7 MPa1990 psi
Elongation at Break 52 %52 %
Modulus of Elasticity 23.4 GPa3390 ksi
Bulk Modulus 15.2 GPa2200 ksi
Poissons Ratio 0.310.31
Shear Modulus 7.38 GPa1070 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000460 ohm-cm0.00000460 ohm-cm
Magnetic Permeability 1.000031.00003
Magnetic Susceptibility 1.0e-61.0e-6cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 216.4 J/g93.10 BTU/lb
Heat of Vaporization 4660 J/g2000 BTU/lb
CTE, linear  22.15 µm/m-°C
@Temperature 20.0 °C
12.31 µin/in-°F
@Temperature 68.0 °F
 22.3 µm/m-°C
@Temperature 0.000 - 400 °C
12.4 µin/in-°F
@Temperature 32.0 - 752 °F
 33.6 µm/m-°C
@Temperature 467 - 603 °C
18.7 µin/in-°F
@Temperature 873 - 1120 °F
 73.3 µm/m-°C
@Temperature 839 - 1382 °C
40.7 µin/in-°F
@Temperature 1540 - 2520 °F
Liquid
Specific Heat Capacity  0.6315 J/g-°C
@Temperature 25.0 °C
0.1509 BTU/lb-°F
@Temperature 77.0 °F
 0.6549 J/g-°C
@Temperature 127 °C
0.1565 BTU/lb-°F
@Temperature 261 °F
 0.7308 J/g-°C
@Temperature 839 °C
0.1747 BTU/lb-°F
@Temperature 1540 °F
liquid
 0.7308 J/g-°C
@Temperature 1027 °C
0.1747 BTU/lb-°F
@Temperature 1881 °F
 0.732 J/g-°C
@Temperature 448 °C
0.175 BTU/lb-°F
@Temperature 838 °F
bcc
 0.7375 J/g-°C
@Temperature 327 °C
0.1763 BTU/lb-°F
@Temperature 621 °F
 0.8079 J/g-°C
@Temperature 448 °C
0.1931 BTU/lb-°F
@Temperature 838 °F
fcc
 0.9174 J/g-°C
@Temperature 627 °C
0.2193 BTU/lb-°F
@Temperature 1160 °F
 1.136 J/g-°C
@Temperature 839 °C
0.2715 BTU/lb-°F
@Temperature 1540 °F
bcc
Thermal Conductivity 126 W/m-K874 BTU-in/hr-ft²-°F
Melting Point 837 - 841 °C1540 - 1550 °F
Boiling Point 1484 °C2703 °F
 
Component Elements PropertiesMetricEnglishComments
Calcium, Ca 100 %100 %
 
Descriptive Properties
CAS Number7740-70-2

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Calcium, Ca; Rolled
Silver, Ag
Americium, Am
Aluminum, Al
Gold, Au

AMECa01 / 17

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.