MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ensinger TECACOMP PEEK 150 GF30 natural 1015097 Polyetheretherketone, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes:
  • high strength
  • high stiffness
  • very high creep resistant
  • high heat deflection temperature
  • very good chemical resistance
  • hydrolysis and superheated steam resistant
  • high dimensional stability
  • low moisture absorption
Target Industries:
  • automotive industry
  • business machines
  • mechanical engineering
  • precision engineering

Information provided by Ensinger Inc.

Vendors: Ensinger TECACOMP compounds withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inDIN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inDIN EN ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 205 MPa29700 psiDIN EN ISO 527-1
Elongation at Break 2.7 %2.7 %DIN EN ISO 527-1
Modulus of Elasticity 11.1 GPa1610 ksiDIN EN ISO 527-1
Charpy Impact Unnotched 6.50 J/cm²30.9 ft-lb/in²DIN EN ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °FDIN 53765
Maximum Service Temperature, Air 260 °C500 °Flong term
 300 °C572 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 330 °C626 °FISO-R 75 Method A
Glass Transition Temp, Tg 143 °C289 °FDIN 53765
 
Processing PropertiesMetricEnglishComments
Processing Temperature 360 - 410 °C680 - 770 °F
Mold Temperature 170 - 210 °C338 - 410 °F
Drying Temperature 150 - 160 °C302 - 320 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
 
Descriptive Properties
Colornatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIO9052 / 318980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.