MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECATRON SX natural Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes:
  • good heat deflection temperature
  • good chemical resistance
  • resistance against high energy radiation
  • high strength
  • high dimensional stability
  • high stiffness
  • high creep resistance
Target Industries:
  • semiconductor technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³
Water Absorption 0.010 %
@Time 86400 sec
0.010 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 103.9103.9ISO 2039-1
Hardness, Shore D 85.285.2ASTM D 2240
Tensile Strength at Break 97.9 MPa14200 psiASTM D638
Tensile Strength, Yield 104.2 MPa15120 psiASTM D638
Elongation at Break 4.98 %4.98 %ASTM D638
Modulus of Elasticity 4.122 GPa597.8 ksiASTM D638
Flexural Strength 154 MPa22400 psiASTM D790
Flexural Modulus 4.115 GPa596.8 ksiASTM D790
Compressive Yield Strength 141.8 MPa
@Strain 10 %
20560 psi
@Strain 10 %
ASTM D695
Compressive Strength 30.17 MPa
@Strain 1 %
4376 psi
@Strain 1 %
ASTM D695
Compressive Modulus 2.961 GPa429.4 ksiASTM D695
Izod Impact, Notched 0.310 J/cm0.580 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmDIN IEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmDIN IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  59.9 µm/m-°C
@Temperature 22.8 - 60.0 °C
33.3 µin/in-°F
@Temperature 73.0 - 140 °F
DIN EN ISO 11359-1;2
 70.0 µm/m-°C
@Temperature 22.8 - 100 °C
38.9 µin/in-°F
@Temperature 73.0 - 212 °F
DIN EN ISO 11359-1;2
 120 µm/m-°C
@Temperature 100 - 150 °C
66.7 µin/in-°F
@Temperature 212 - 302 °F
DIN EN ISO 11359-1;2
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°FISO 22007-4:2008
Thermal Conductivity 0.251 W/m-K1.74 BTU-in/hr-ft²-°FISO 22007-4:2008
Melting Point 284 °C543 °F
Maximum Service Temperature, Air 230 °C446 °Flong term
 260 °C500 °Fshort term
Glass Transition Temp, Tg 172 °C341 °F
Flammability, UL94 HBHBDIN IEC 60695-11-10
 
Descriptive Properties
Colorbeige opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8235 / 319163

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.