MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxygen-free high conductivity Copper, Hard, UNS C10200
Categories: Metal; Nonferrous Metal; Copper Alloy; Wrought Copper

Material Notes: Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass to metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.

Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping.

Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.

Forms: pipe, plate, rod, shapes, sheet, strip, tube, and wire.

UNS C10200 - ASTM (flat products) B48, B133, B152, B187, B272, B370, B432, B451, (pipe) B42, B188, (rod) B12, B49, B124,B133, B187, (tubing) B68, B75, B88, B111, B188, B280, B359, B372, B395, B447, (shapes) B124,B133, B187, (wire) B1, B2, B3, B33, B47, B116, B189, B246, B286, B298, B355; C103 (UK); CDA 102 OF; CEN CW009A; Cu/cl NF A53301 (France), ISO Cu-OF R1337; JIS C1020 H3100 - sheet, plate, C1020 H3140 - bar (Japan); QQ-C-576 (flat products), QQ-C-502 (rod, shapes); QQ-C-576 (tube); QQ-C-502, QQ-W-343, MIL-W-3318 (wire)

Key Words: ASTM B1, B2, B3, B12, B33, B42, B47, B48, B49, B68, B75, B88, B111, B116, B124, B133, B152, B187, B188, B189, B246, B272, ASTM B286, B298, B355, B359, B370, B372, B395, B432, B451, B447, C103, CDA 102 OF, CEN CW009A, Cu/cl NF A53301, QQ-C-576, CDA 102 OF, C103, ISO Cu-OF R1337, CEN CW008A
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 261 - 441 MPa37900 - 64000 psiVaries with heat treatment
Tensile Strength, Yield 88.0 - 324 MPa
@Strain 0.1 %
12800 - 47000 psi
@Strain 0.1 %
varies with temper and cold work.
Elongation at Break 6.0 - 30 %6.0 - 30 %
Modulus of Elasticity 117 - 132 GPa17000 - 19100 ksi
Poissons Ratio 0.310.31
Machinability 20 %20 %Based on 100% machinability for BS2874 CZ 121 Free-machining brass (20% of 100% for UNS C360000)
Forgeability 65 %65 %
Shear Modulus 44.0 GPa6380 ksi
Izod Impact 34.0 - 61.0 J25.1 - 45.0 ft-lbType of Impact test unknown. Range reflects both soft and hard tempers.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000169 - 0.00000173 ohm-cm
@Temperature 20.0 °C
0.00000169 - 0.00000173 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.61 µin/in-°F
@Temperature 68.0 - 392 °F
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C
@Temperature 20.0 °C
0.0920 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 391 W/m-K
@Temperature 20.0 °C
2710 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1083 °C1981 °F
Annealing Point >= 371 °C>= 700 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.95 %>= 99.95 %includes silver (minimum 99.95% Cu+Ag)

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxygen-free high conductivity Copper, Soft, UNS C10200
Oxygen-free electronic Copper, UNS C10100
Oxygen-free Copper (OF), UNS C10200, H00 Temper, flat products
Oxygen-free Electronic Copper (OFE), UNS C10100, H00 Temper, flat products
Copper, Cu; Annealed

MC10200b2 / 10338

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.