MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SCG Chemicals SG66Z PVC Resin Powder
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Powder

Material Notes: Polyvinyl Chloride Homopolymer having medium molecular weight, is white and free-flowing resins produced by suspension polymerization process. The resin can easily blend with variety of additives to achieve desired qualities needed in many applications. Applications are ranging from general purpose to special products regarding customer's satisfactions.

Applications: Transparent Sheet, Electrical Taper, Artificial Leather, Other Flexible, Films and Sheets, Furniture and Automotive Trim, Flexible Hose, Electrical Wire and Cable, Stretch Film, Other Rigid and Soft Profiles., Toy, Other Rigid and Flexible Products.

Features: Good initial coloration. Good thermal stability.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.520 g/cc0.0188 lb/in³ISO-60
Volatiles <= 0.30 %<= 0.30 %ISO-1269
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 3.00e+13 ohm-cm>= 3.00e+13 ohm-cmTPC Method
 
Descriptive Properties
AppearanceWhite powder
Fish Eye (Point)<5 point/150 cm2TPC Method
Impurity and Foreign Matter<5 specks/100sqISO/R-1265
K Value66ISO 1628-2. Corresponding polymerization degree= 1000.
Residual VCM (ppm)<1ASTM D3749
Sieve Analysis (%)>90ASTM D1921. Retained on 75 micron.
 0ASTM D1921. Retained on 250 micron.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCGC847 / 278104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.