MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman BMC 5592 Arc, Track, and Weather Resistant Polyester
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame resistance and electrical characteristics.

Typical applications include third rail and other rapid transit insulators.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.87 g/cc1.87 g/cc
Water Absorption 0.10 %0.10 %24 hours, 23°C
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 35 - 4535 - 45
Tensile Strength, Ultimate 68.9 - 89.6 MPa10000 - 13000 psi
Flexural Strength 159 - 186 MPa23000 - 27000 psi
Compressive Strength 152 - 165 MPa22000 - 24000 psi
Izod Impact, Notched 6.94 - 8.01 J/cm13.0 - 15.0 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 14.6 - 15.7 kV/mm370 - 400 kV/inShort Time
Arc Resistance 195 sec195 sec
Track Resistance >= 60000 sec>= 60000 secinclined plane, 2500 volts
Comparative Tracking Index >= 600 V>= 600 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °F
Flammability, UL94  V-0
@Thickness 6.35 mm
V-0
@Thickness 0.250 in
 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 V-0
@Thickness 1.02 mm
V-0
@Thickness 0.0400 in
Flammability Test 5050burn time, [sec]
 200200ignition time, [sec]
 
Processing PropertiesMetricEnglishComments
Mold Temperature 138 - 166 °C280 - 330 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBMC068 / 27251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.