MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SEKISUI SPI ALLEN® 752 ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: High Impact ABS Sheet (High Gloss)

ALLEN® 752 is a high gloss, high impact, FDA approved, general purpose ABS with excellent low temperature performance.

ALLEN® 752 is Underwriters Laboratories, Inc® recognized for UL Std 94 HB (UL94) and Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302), and US Food and Drug Administration CFR 181.32 (Acrylonitrile copolymers and resins).

Suggested Applications:

  • Mechanical covers & housings
  • Beverage dispensers
  • Ice bins
  • Food equipment

Features:

  • Custom color matching
  • Good forming properties
  • Edge trim easily used into future orders
  • High gloss
  • Excellent low temperature performance
  • High impact
  • FDA 21 CFR, 181.32 compliant

Information provided by Sekisui Polymer Innovations

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Tensile Strength 35.1 MPa5090 psiASTM D638
Flexural Strength 55.1 MPa7990 psiASTM D790
Flexural Modulus 1.8616 GPa270.00 ksiASTM D790
Izod Impact, Notched  2.08 J/cm
@Temperature -17.8 °C
3.90 ft-lb/in
@Temperature 0.000 °F
ASTM D256
 3.36 J/cm
@Temperature 22.8 °C
6.29 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Transverse to Flow 93.6 µm/m-°C52.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C210 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
Underwriters Laboratories., Inc®; Component Recognition; UL Standard 94
 
Optical PropertiesMetricEnglishComments
Gloss 90 %90 %60° Angle; ASTM D523
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Motor Vehicle Safety StandardPassesFMVSS 302

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade
Hannam Chemical Hanalac 750 ABS, General Purpose
PTS Trilac® ABS-HS6500 High Impact ABS Resin
RTP Company RTP 600 Z  Acrylonitrile Butadiene Styrene (ABS) FDA Type
SEKISUI SPI ALLEN® 3800/LXS ABS

PSEKIS005 / 185830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.