MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Angst+Pfister APSOplast® PET-A Amorphous PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: PET-A is a transparent polyester material with a high translucency and surface gloss. It is particularly characterized by high dielectric strength and break resistance along with excellent cold-bending properties. PET-A has a good UV- and chemical resistance and is suitable for use in the food industry. PET-A is flame-retardant as per Fire Class B1 in accordance with DIN 4102 and is tested for rail vehicles in accordance with DIN 5510 (S4, SR2, and ST2).

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³DIN EN ISO 1183-1
Moisture Absorption 0.500 %0.500 %50 % r.h.; DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 55.0 MPa>= 7980 psi50 mm/min; DIN EN ISO 527
Tensile Strength, Yield >= 55.0 MPa>= 7980 psi50 mm/min; DIN EN ISO 527
Elongation at Break >= 25 %>= 25 %50 mm/min; DIN EN ISO 527
Elongation at Yield 4.0 %4.0 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 2.50 GPa363 ksi1 mm/min; DIN EN ISO 527
Charpy Impact Unnotched NBNBDIN EN ISO 179-1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant 3.43.4IEC 60250
Dielectric Strength 60.0 kV/mm1520 kV/inIEC 60243
Dielectric Loss Index 0.0150.015IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C27.8 µin/in-°FDIN 53752
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 60.0 °C140 °F
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C145 °FDIN EN ISO 75
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5871.587ISO 489
Transmission, Visible 87 %
@Thickness 3.00 mm
87 %
@Thickness 0.118 in
DIN 5036 / ASTM D-1003 / ISO 13468-1/-2
 
Descriptive Properties
Colorclear transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP018 / 250516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.