MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gharda Chemicals GAFONE™-P 4300 PPSU, High Impact Strength, High Hydrolysis Resistance  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Neat grade suitable for extrusion, injection molding, blow molding and thermoforming.

Characteristics:

  • Outstanding impact resistance
  • Outstanding resistance to hydrolysis and sterilization
  • Very good solvent resistance
  • Good flame resistance

Applications:

  • Medical applications
  • Interior panels in air and surface transportation

Information provided by Gharda.

Solvay Advanced Polymers completed its acquisition of this product line in May 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.38 %0.38 %ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cm0.0050 - 0.0060 in/inASTM D955
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 400 °C
10 g/10 min
@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psiASTM D638
Elongation at Break 8.0 %8.0 %ASTM D638
Tensile Modulus 2.40 GPa348 ksiASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 2.30 GPa334 ksiASTM D790
Izod Impact, Notched 6.50 J/cm12.2 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
Dielectric Constant 3.23.2
Dielectric Strength 18.0 kV/mm457 kV/inASTM D149
Arc Resistance 70 sec70 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 185 °C365 °FContinuous use, UL
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Overview of materials for Polyphenylsulfone (PPSU)
Ensinger RADEL® R-5500 Polyphenylsulfone (PPSU)
Ensinger TECASON™ P Polyphenylsulfone (PPSU)
Envalior Stanyl® TW200B6 PA46-CF30, Dry, 30% Carbon Reinforced, Heat Stabilized

PGHARDA12 / 41787

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.