MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lithium, Li
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.530 g/cc0.0191 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 6.9416.9411995
Atomic Number 33
Thermal Neutron Cross Section 70 barns/atom70 barns/atom
X-ray Absorption Edge 226.62 Å226.62 ÅK
Critical Temperature 2950 °C5340 °F
Electrode Potential -3.02 V-3.02 V
Electronegativity 0.980.98Pauling
Ionic Radius 0.680 Å0.680 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 0.262 g/A/h0.262 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers <= 5.0<= 5.0
Tensile Strength, Ultimate <= 15.0 MPa<= 2180 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000840 ohm-cm0.00000840 ohm-cm
Magnetic Susceptibility 5.0e-75.0e-7cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 137 J/g58.9 BTU/lb
Heat of Vaporization 19460 J/g8372 BTU/lb
CTE, linear 56.0 µm/m-°C
@Temperature 20.0 - 100 °C
31.1 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 2.997 J/g-°C0.7162 BTU/lb-°FGas
 3.305 J/g-°C0.7899 BTU/lb-°F
Thermal Conductivity 71.2 W/m-K494 BTU-in/hr-ft²-°F
Melting Point 180.54 °C356.97 °F
Boiling Point 1342 °C2448 °F
Heat of Formation 159.3 kJ/mol159.3 kJ/molGas
 
Component Elements PropertiesMetricEnglishComments
Lithium, Li 100 %100 %
 
Descriptive Properties
CAS Number7439-93-2
SolubilityReacts with H2O

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum, Al
Silver, Ag
Titanium, Ti
Iron, Fe
Sandstone, Soft

AMELi00 / 54

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.