MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

E-CRGlas® Fiber
Categories: Ceramic; Glass; Glass Fiber; Oxide; Silicon Oxide; Other Engineering Material; Composite Fibers

Key Words: GRP composites, fiber glass composites, single fiber, FRP composites
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.72 g/cc0.0983 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3445 MPa499700 psi
 5310 MPa
@Temperature -190 °C
770000 psi
@Temperature -310 °F
Elongation at Break 4.8 %4.8 %
Modulus of Elasticity 72.3 GPa10500 ksi
 81.3 GPa
@Temperature 540 °C
11800 ksi
@Temperature 1000 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.84e+12 ohm-cm3.84e+12 ohm-cm
Dielectric Constant 6.9
@Frequency 1e+6 Hz
6.9
@Frequency 1e+6 Hz
Dielectric Strength 9.80 kV/mm249 kV/in
Dissipation Factor  0.0028
@Frequency 1e+6 Hz
0.0028
@Frequency 1e+6 Hz
 0.0031
@Frequency 60 Hz
0.0031
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.90 µm/m-°C
@Temperature 20.0 °C
3.28 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.970 J/g-°C
@Temperature 200 °C
0.232 BTU/lb-°F
@Temperature 392 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5791.579
 1.5831.583bulk annealed
 1.5831.583bulk annealed

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
AR-Glass Fiber, Generic
S-2 Glass® Fiber
AGY ADVANTEX® Generic Glass Fiber
R-Glass Fiber, Generic

CGF008 / 904

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.