MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Petra® 140 45% Glass Filled PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 50% Glass Reinforced

Material Notes: Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Excellent resistance to creep under load, and maintains the inherent chemical and electrical properties associated with polyesters.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Melt Density 1.44 g/cc
@Temperature >=245 °C
0.0520 lb/in³
@Temperature >=473 °F
ISO 1183
Viscosity Measurement 0.520.52Inherent Viscosity
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 116116ASTM Test
Tensile Strength at Break 180 MPa26100 psi0.2 in/min; ASTM Test
Tensile Strength, Ultimate 180 MPa26100 psi5mm/min; ISO 527
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527
 3.0 %3.0 %0.2 in/min; ASTM Test
Tensile Modulus 16.2 GPa2350 ksi1mm/min; ISO 527
Flexural Strength 255 MPa37000 psiISO Data
 285 MPa41300 psiASTM Test
 110 MPa
@Temperature 120 °C
16000 psi
@Temperature 248 °F
ASTM Test
 370 MPa
@Temperature -40.0 °C
53700 psi
@Temperature -40.0 °F
ASTM Test
Flexural Modulus 13.1 GPa1900 ksiASTM Test
 4.69 GPa
@Temperature 120 °C
680 ksi
@Temperature 248 °F
ASTM Test
Izod Impact, Notched 1.10 J/cm
@Thickness 3.17 mm
2.06 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Unnotched 9.60 J/cm18.0 ft-lb/inASTM Test
Charpy Impact, Notched 1.15 J/cm²5.47 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear 22.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
12.2 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
CTE, linear, Parallel to Flow 22.0 µm/m-°C12.2 µin/in-°FASTM Test
Specific Heat Capacity 1.573 J/g-°C0.3760 BTU/lb-°FMelt
Thermal Conductivity 0.310 W/m-K2.15 BTU-in/hr-ft²-°FMelt
Melting Point 245 °C473 °F10 K/min
 245 °C473 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 242 °C468 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75
 225 °C437 °FASTM Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 275 °C527 °FInjection molding
Mold Temperature 115 °C239 °FInjection molding
Injection Velocity 115 mm/sec4.53 in/secInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET
Celanese Rynite® 545 BK504 PET-GF45
BASF Petra® 110 BK-112 15% Glass Filled PET
BASF Petra® 130 30% Glass Filled PET
BASF Capron® SEGM35H1 BK-126 15/25% Glass/Mineral-Filled Nylon 6 (Dry)

PBASF9020 / 84784

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.