MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Delrin® DE9156 NC010 , High Viscosity Acetal with Teflon® PTFE Micropowder  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, PTFE-Filled

Material Notes: High Viscosity Acetal Resin with Teflon® PTFE Micropowder Resin

Specifications: Mechanical properties measured at 23°C unless otherwise noted.

Comments: Processing Moisture Content: 0.2% Max. Hold Pressure Range: 70-100 MPa.

Data provided by DuPont Engineering Polymers for the European and Asia Pacific regions.

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Melt Flow 2.2 g/10 min2.2 g/10 min190°C, 2.16 kg; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 71.0 MPa10300 psiISO 527-1/-2
Elongation at Break 30 %30 %nominal; ISO 527-1/-2
 50 %50 %ISO 527-1/-2
Elongation at Yield 22 %22 %ISO 527-1/-2
Modulus of Elasticity 3.10 GPa450 ksiISO 527-1/-2
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 177 °C351 °FISO 3146C
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 220 °C410 - 428 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2 hour2 hour
Moisture Content <= 0.20 %<= 0.20 %
Injection Pressure 70.0 - 100 MPa10200 - 14500 psiHold Pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF065 / 32669

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.