MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Torlon® 7130 PAI, 30% carbon fiber
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: 30% carbon fiber, best stiffness, best retention of stiffness at high temperatures, best fatigue resistance, electrically conductive

Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal expansion characteristics similar to steel, and therefore excellent dimensional stability.

Torlon® PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals.

The potential applications for this resin include metal replacement, sliding vanes, aerospace parts, impellors, shrouds, pistons, and housings.

It is available in injection molding and extrusion (E) grades.

Markets/Uses: Aircraft / Mechanical & Structural Applications / Brackets and Hinges; Aircraft / Mechanical & Structural Applications / Engine Components; Aircraft / Mechanical & Structural Applications / Engine Fan Cowling Vents; Aircraft / Mechanical & Structural Applications / Fan Impeller; Aircraft / Mechanical & Structural Applications / Mounting Support Rails; Aircraft / Mechanical & Structural Applications / Seals; Aircraft / Mechanical & Structural Applications / Stock Shapes for Prototyping; Aircraft / Mechanical & Structural Applications / Support Brackets; Automotive / Mechanical & Structural Parts / Gears; Films / High Temperature Films / Brackets and Hinges; Films / High Temperature Films / Engine Components; Films / High Temperature Films / Engine Fan Cowling Vents; Films / High Temperature Films / Fan Impeller; Films / High Temperature Films / Mounting Support Rails; Films / High Temperature Films / Seals; Films / High Temperature Films / Stock Shapes for Prototyping; Miscellaneous / Industrial / Compressor Components; Oil & Gas / Down Hole / Back-Up Seal Rings; Oil & Gas / Down Hole / Compressor Components; Oil & Gas / Down Hole / Down Hole Connectors; Oil & Gas / Down Hole / Electrical Connectors; Oil & Gas / Down Hole / Motor End Plate; Oil & Gas / Down Hole / Poppets; Semiconductor / Fabrication & Testing / Mechanical Fasteners

Applications: Aerospace Applications; Aircraft Applications; Business Equipment; Connectors; Electrical/Electronic Applications; Film; Gears; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Oil/Gas Applications; Semiconductor Molding Compounds

Features: Chemical Resistant; Creep Resistant; Fatigue Resistant; Flame Retardant; Good Compressive Strength; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Temperature Strength; Semi Conductive

Injection notes: Minimum drying conditions: 3 hours at 350°F (177°C), 4 hours at 300°F (149°C), or 16 hours at 250°F (121°C).
Compression Ratio: 1:1 to 1.5:1
Begin hold pressure at a high setting 6,000-8,000 psi (41.37-55.16 MPa), for several seconds, then drop off to 3,000-5,000 psi (20.69-34.48 MPa), for the duration of the hold pressure sequence.
Molded parts must be post cured.

Information provided by Solvay Specialty Polymers.

Vendors: Drake Plastics Ltd. Co. The Torlon Specialist, manufactures & stocks the most complete line of Torlon PAI in machinable rod, plate & Seamless Tube®. Drake works closely with Solvay Specialty Polymers to identify & serve a multitude of new applications. Drake, a lean producer of extruded, injection molded & machined shapes & parts, offers low minimums & quick, economical delivery globally.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ASTM D792
Water Absorption 0.26 %
@Time 86400 sec
0.26 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow <= 0.0015 cm/cm<= 0.0015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 221 MPa32100 psiASTM D638
Tensile Stress 203 MPa29400 psiASTM D1708
Tensile Modulus 16.5 - 22.3 GPa2390 - 3230 ksiASTM D638
Flexural Strength 350 MPa50800 psiASTM D790
Flexural Modulus  15.7 GPa
@Temperature 232 °C
2280 ksi
@Temperature 450 °F
ASTM D790
 19.9 GPa
@Temperature 23.0 °C
2890 ksi
@Temperature 73.4 °F
ASTM D790
Compressive Strength 254 MPa36800 psiASTM D695
Compressive Modulus 9.86 GPa1430 ksiASTM D695
Izod Impact, Notched 0.480 J/cm0.899 ft-lb/inASTM D256
Izod Impact, Unnotched 3.20 J/cm5.99 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FASTM D696
Thermal Conductivity 0.520 W/m-K3.61 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 282 °C540 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 304 °C579 °F
Nozzle Temperature 371 °C700 °F
Mold Temperature 199 - 216 °C390 - 421 °F
Drying Temperature 177 °C
@Time 10800 sec
351 °F
@Time 3.00 hour
Moisture Content <= 0.050 %<= 0.050 %Injection
Back Pressure 6.89 MPa999 psi
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsPellets
ProcessingInjection Molding; Machining; Profile Extrusion
RoHS ComplianceYes
Screw L/D Ratio, Injection18.0:1.0 to 24.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4552 / 280352

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.