MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals Novapol® TR-0740-U Hexene Copolymer MDPE Rotational Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded

Material Notes: Features: good impact properties, excellent processability, NSF listed for standards #51, 61, UL 94HB. Additives: processing antioxidant, UV stabilizer (estimated UV resistance UV8).

Applications: part light weighting, toys, complex custom parts, home and garden items, mailboxes.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D 792
ESCR 100% Igepal® 110 hour110 hourCondition B, (F50); ASTM D1693
Melt Index of Compound 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.6 MPa
@Thickness 1.90 mm
2990 psi
@Thickness 0.0748 in
Type IV specimen, 2" (50.8 mm) per minute test speed, compression molded.; ASTM D638
Elongation at Yield 12 %
@Thickness 1.90 mm
12 %
@Thickness 0.0748 in
Type IV specimen, 2" (50.8 mm) per minute test speed, compression molded.; ASTM D638
Flexural Modulus 0.915 GPa
@Strain 1 %
133 ksi
@Strain 1 %
Compression molded; ASTM D790
Impact Test  61.0 J
@Thickness 3.17 mm,
Temperature -40.0 °C
45.0 ft-lb
@Thickness 0.125 in,
Temperature -40.0 °F
ARM test; rotomolded samples.
 197 J
@Thickness 6.35 mm,
Temperature -40.0 °C
145 ft-lb
@Thickness 0.250 in,
Temperature -40.0 °F
ARM test; rotomolded samples.
 
Thermal PropertiesMetricEnglishComments
Melting Point 126 °C259 °FDSC.
Heat Distortion Temperature  42.0 °C
@Pressure 1.82 MPa
108 °F
@Pressure 264 psi
ASTM D648
 60.0 °C
@Pressure 0.455 MPa
140 °F
@Pressure 66.0 psi
ASTM D648
Flammability, UL94 HBHB
 
Compliance PropertiesMetricEnglishComments
NSF YesYesstandards #51, 61

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOV614 / 249061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.