MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxygen-free Copper (OF), UNS C10200, OS050 temper, flat products, rod, tubing, and shapes
Categories: Metal; Nonferrous Metal; Copper Alloy; Wrought Copper

Material Notes: Test specimens: flat product, 1 mm thick.; rod, 25 mm (1 in) diam.; tubing, 25 mm (1 in) diam., 1.65 (0.065 in) mm wall thickness; shape, 13 mm (0.50 in) section.

Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass-to-metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.

Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, shearing, spinning, swaging, and stamping.

Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.

UNS C10200 - ASTM (flat products) B48,B133, B152, B187, B272, B370, B432; (rod) B12, B49, B124,B133, B187; (tubing) B68, B75, B88, B111, B188, B280, B359, B372, B395, B447; (shapes) B124,B133, B187; C103 (UK); CDA 102 OF; CEN CW009A; ISO Cu-OF R1337; JIS C1020 H3100 (sheet, plate) (Japan); QQ-C-576

Key Words: BS C110, C103, ISO Cu-OF R1337, CEN CW009A, oxygen free high conductivity copper (OFHC), CDA 102 OF, ASTM B48, B133, B152, B187, B272, B370, B432, Cu/cl NF A53301, C1020 H3100, C1020 H3140, flat products, plates, sheets, strips, QQ-C-576
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 4040Flat products, rod, and tubing
 5555Rod, 70% reduction in area
Tensile Strength, Ultimate 220 MPa31900 psi
Tensile Strength, Yield 69.0 MPa
@Strain 0.5 %
10000 psi
@Strain 0.5 %
Elongation at Break  45 %
@Thickness 1.00 mm
45 %
@Thickness 0.0394 in
flat specimen, tubing
 50 %
@Thickness 6.00 mm
50 %
@Thickness 0.236 in
shapes
Reduction of Area 55 %55 %in 25 mm (1 in) rod specimen
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.310.31
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %65 %UNS C37700 (forging brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 150 MPa21800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000171 ohm-cm
@Temperature 20.0 °C
0.00000171 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.61 µin/in-°F
@Temperature 68.0 - 392 °F
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C
@Temperature 20.0 °C
0.0920 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 391 W/m-K
@Temperature 20.0 °C
2710 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1083 °C1981 °F
Annealing Point >= 371 °C>= 700 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 375 - 650 °C707 - 1200 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.95 %>= 99.95 %includes silver (minimum 99.95% Cu+Ag)

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxygen-free Copper (OF), UNS C10200, H80 (40%) rod, tubing (25 mm o.d. and 1.65 wall thickness)
Oxygen-free Copper (OF), UNS C10200, O61 Temper Bar
Oxygen-free Copper (OF), UNS C10200, OS025 temper, flat products and tubing
Oxygen-free Copper (OF), UNS C10200, H10 Temper, flat products
Oxygen-free Copper (OF), UNS C10200, H55 (15%) temper, tubing

MC10200d1 / 10376

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.