MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Calcium S NLGI Grade 2
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Calcium S is a high-quality, extreme-pressure (EP) calcium stearate grease specially developed for use by automobile manufacturers and parts suppliers to the automobile industry. It is recommended for the lubrication of window regulators, door hinges and similar automotive hardware. Calcium S is manufactured with high-quality, low-viscosity base oils and a calcium stearate soap thickener. It is fortified with extreme-pressure and antiwear additives, plus rust and oxidation inhibitors. It has excellent oxidation resistance for long service life, has good load-carrying capacity for protection against wear, and protects metal parts against rust and corrosion. It has good resistance to water washout, and excellent low-temperature pumpability.

Applications:

  • Window regulators, door hinges and similar hardware on automotive vehicles
  • Sliding mechanisms on automobile seats
  • Industrial equipment where a water-resistant, extreme pressure calcium grease with excellent low-temperature pumpability is recommended
Calcium S is recommended for use where the OEM specifies:
  • Ford WSB-M1C163-D
Calcium S is approved by Meritor for use in the manufacture of automotive window regulators.

Features/Benefits:

  • Excellent oxidation resistance
  • Good load-carrying capacity
  • Good wear protection
  • Protects against rust and corrosion
  • Good resistance to water washout
  • Excellent low-temperature pumpability
  • Excellent storage stability

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³
Viscosity Measurement 5858Index
Saybolt Viscosity at 100°F 83 SUS83 SUS
Saybolt Viscosity at 210°F 37 SUS37 SUS
Kinematic Viscosity at 40°C (104°F) 15.1 cSt15.1 cSt
Kinematic Viscosity at 100°C (212°F) 3.2 cSt3.2 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
100 hour
@Pressure 5.00 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)ASTM D2596
Four Ball Wear 0.550 mm0.0217 inScar Diameter; ASTM D2266
Penetration P(60), 1/10 mm 265 - 295265 - 295ASTM D217
Timken Test 20400 g45.0 lbOK Load; ASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 107 °C225 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °F
Dropping Point 140 °C284 °F
 
Descriptive Properties
ColorAmber
ThickenerCalcium Stearate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5108 / 198361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.