MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NX 188 Cast Nickel Superalloy
Categories: Metal; Superalloy; Nickel Base

Material Notes: Directionally Solidified; Typical Applications: Jet engine vanes

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  51.0 MPa
@Temperature 1090 °C,
Time 3.60e+6 sec
7400 psi
@Temperature 2000 °F,
Time 1000 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 82.7 MPa
@Temperature 1090 °C,
Time 360000 sec
12000 psi
@Temperature 2000 °F,
Time 100 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 128 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
18500 psi
@Temperature 1800 °F,
Time 1000 hour
Estimated from limited data using the Larson-Miller time-temperature parameter
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.0 %8.0 %
Carbon, C 0.040 %0.040 %
Nickel, Ni 91.96 %91.96 %As Balance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Nistelle Super C Nickel Superalloy
IN-162 Cast Nickel Superalloy
DS-Niclel Nickel Superalloy Sheet
B. 1900 Cast Nickel Superalloy
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal

NZ97032 / 191432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.