MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Kendall® SHP® Grease NLGI Grade 2
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Kendall® SHP Grease is a premium quality, multipurpose, extreme-pressure (EP) calcium sulfonate grease specially developed for use in industrial and automotive equipment operating in wet or corrosive environments. It is particularly recommended for equipment exposed to water contamination, saltwater corrosion and/or high temperatures. SHP Grease is manufactured with high-quality base oils and a non-soap, calcium sulfonate thickener. It is fortified with antiwear additives and rust and corrosion inhibitors. It protects against rust and corrosion in high-humidity, high-temperature applications such as those found in the steel, lumber, tire manufacturing and paper industries. It has excellent load-carrying capacity, high shear stability and outstanding resistance to water washout. SHP Grease is NLGI GC-LB certified for use as a multipurpose automotive wheel bearing and chassis lubricant.

Applications:

  • Industrial and automotive equipment operating at high temperatures and exposed to water contamination, high humidity or corrosive environmental conditions
  • Chassis parts and wheel bearings on heavy-duty and fleet equipment
  • Marine equipment, heavy mobile equipment and cables exposed to salt water
  • Paper machine wet- and dry-end bearings and hot calendar stacks
  • Rolling mills, hot roll tables, continuous casters, ingot buggies and slab mills
  • Steel mill roller bearings, conveyors and gears
  • Centralized lube systems and auto lubbers in service shops
Features/Benefits:
  • Excellent oxidation resistance and thermal stability at high temperatures
  • Outstanding rust and corrosion protection, including resistance to saltwater corrosion
  • Excellent extreme-pressure and antiwear properties
  • High load-carrying capacity
  • Outstanding resistance to water washout
  • Excellent shear stability
  • NLGI GC-LB certified

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³
Viscosity Measurement 9797Index
Saybolt Viscosity at 100°F 522 SUS522 SUS
Saybolt Viscosity at 210°F 65 SUS65 SUS
Kinematic Viscosity at 40°C (104°F) 100 cSt100 cSt
Kinematic Viscosity at 100°C (212°F) 11.2 cSt11.2 cSt
Oxidative Stability 100 hour
@Pressure <=0.00689 MPa
100 hour
@Pressure <=1.00 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 500 kg1100 lb (mass)ASTM D2596
Four Ball Wear 0.390 mm0.0154 inScar Diameter; ASTM D2596
Penetration 265 - 295265 - 295Worked
Timken Test 29500 g65.0 lbASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -34.0 °C-29.2 °F
Dropping Point 290 °C554 °F
 
Descriptive Properties
ColorRed
ThickenerCalcium Sulfonate
Water Washout Resistance0.028ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5328 / 198581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.