MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 8503-5/AboCure 8503-5 Colorless Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: AboCast 8503-5/AboCure 8503-5 is a faster hardening, colorless epoxy casting compound used for small castings and decoupage. It is a good choice for small castings, especially for analytical purposes and for small embedments, due to its faster reactivity. Suggested Uses: Transparent Casting, Embedding, Encapsulation, Potting, and Bonding. Casting display or experimental models without the high shrinkage of acrylic or other resins. Precise reproduction of anatomical or scientific models. Embedding organic, geologic, or metallurgic specimens. Encapsulation of electric, radioactive, or delicate components. Preservation or repair of artistic and historical objects. High-performance transparent table tops.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1100 cP1100 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8181
Tensile Strength at Break 56.5 MPa8200 psi
Elongation at Break 15 %15 %
Flexural Strength 77.9 MPa11300 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 50.0 °C122 °FDeflection Temp at unknown load
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Pot Life 30 min
@Temperature 25.0 °C
30 min
@Temperature 77.0 °F
500 g
 
Descriptive Properties
Hardening Time (min)60-480
Parts by Weight (pbw)100AboCast
 80AboCure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resinlab® EP1330LV Heat Cure Epoxy Polymer System
Resinlab® EP1330 Heat Cure Epoxy Polymer System
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
Lord Adhesives Thermoset™ ME-430 Epoxy Board Level Encapsulant
Epoxy Technology EPO-TEK® E3037 Epoxy

PABC891 / 107875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.