Data provided by the supplier, MarkeTech International. These materials are epi ready and are also available as polycrystal wafers and as seed crystals. Standard orientation: <100> ±20' or 2-3° of <100> toward <110>; 5E+17 EDP/cm²; 5E-17 CC-3; Mobility >1600 cm²/Vs MarkeTech International is no longer in business. |