MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik 19C27 Strip Steel
Categories: Metal; Ferrous Metal; Martensitic; Special-Purpose Steel; Stainless Steel

Material Notes: Sandvik 19C27 is a martensitic stainless chromium steel with a high carbon content. After heat treatment the steel is characterized by:
  • A very high hardness
  • A very good wear resistance
  • This grade is used for the production of industrial knives for cutting synthetic fibre, paper and plastic films.

    Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell B <= 103<= 103annealed
     101.4 - 108.7101.4 - 108.7cold rolled
    Hardness, Rockwell C 5555tempering temperature- 350°C
     61.561.5tempering temperature- 150°C
    Hardness, Vickers <= 275<= 275annealed
     265 - 345265 - 345cold rolled
    Tensile Strength, Ultimate <= 800 MPa<= 116000 psiannealed
     850 - 1000 MPa123000 - 145000 psicold rolled
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C 0.95 %0.95 %
    Chromium, Cr 13.5 %13.5 %
    Iron, Fe 84.5 %84.5 %As Balance
    Manganese, Mn 0.70 %0.70 %
    Phosphorus, P <= 0.025 %<= 0.025 %
    Silicon, Si 0.40 %0.40 %
    Sulfur, S <= 0.010 %<= 0.010 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Sandvik 20C Strip Steel
    Sandvik 12C27 Strip Steel
    AISI 4140H Steel, heat treated, tempered 425°C (800°F), 25 mm (1 in.) round
    Materion Brush 60™ HT
    Sandvik 20C Shock Absorber Strip Steel

    NSANDV282 / 19176

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.