MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestamid® DX9321 Black 20% Glass Reinforced Nylon 612 (DAM)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler

Material Notes: Description: impact-resistant,20% glass fiber reinforced, heat-stabilized

Applications: housings, coverings

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA612-HI, MH, 14-050, GF20
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.80 %0.80 %23°C/50% R.H.; ISO 62
Water Absorption at Saturation 2.0 %2.0 %ISO 62
Linear Mold Shrinkage 0.0066 cm/cm0.0066 in/in127x12.7x3.2 mm (processing cond. acc. To DIN EN ISO 1874-2)
Linear Mold Shrinkage, Transverse 0.0088 cm/cm0.0088 in/in127x12.7x3.2 mm (processing cond. acc. To DIN EN ISO 1874-2)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 109 MPa15800 psiISO 527-2/1A
Elongation at Break 6.0 %6.0 %ISO 527-2/1A
Tensile Modulus 5.45 GPa790 ksiISO 527-2/1A
Charpy Impact Unnotched  9.30 J/cm²
@Temperature 23.0 °C
44.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 10.6 J/cm²
@Temperature -30.0 °C
50.4 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.24 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Dielectric Constant  3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
 4.4
@Frequency 100 Hz
4.4
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.047
@Frequency 1e+6 Hz
0.047
@Frequency 1e+6 Hz
IEC 60250
 0.050
@Frequency 100 Hz
0.050
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VTest Solution A, 50 drops; IEC 60112
 600 V600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal; ISO 11359
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
Melting Point 215 °C419 °FPeak Temperature; ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 208 °C406 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 189 °C372 °FISO 75
Vicat Softening Point 207 °C405 °F50N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamid® DX9321 Black 20% Glass Reinforced Nylon 612 (Conditioned)
A. Schulman BMC 695 Vinyl Ester Molding Compound
Evonik Vestamid® X7380 23% Glass, Antistatic, Black, Electrically Conductive Nylon 12
Evonik Vestamid® DX9323 Black 35% Glass Reinforced Nylon 612 (Dry as Molded)
Arkema Rilsamid® DZM 30 BLACK TL PA612-GF30

PHULA13 / 47373

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.