MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik EUROPLEX® PPSU Sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: EUROPLEX®sheets based on the engineering polymer polyphenyl sulphone (PPSU) are employed worldwide more and more frequently to manufacture visors for the protection of fire workers at their dangerous operations during fire fighting and lifesaving. EUROPLEX® PPSU is a sheet material distinguished by its special combination of properties:
  • EUROPLEX® PPSU is inherently flame-retardant (self-extinguishing without flame retardant). Its rating of UL94:V0 at 0.8 mm thickness stands for very good fire behavior.
  • High heat distortion temperature up to 190°C in permanent service.
  • EUROPLEX® PPSU shows excellent mechanical properties over a wide temperature range – also at low temperatures. Therefore face shields manufactured from this material are virtually unbreakable.
  • Being an amorphous material EUROPLEX® PPSU shows extraordinary chemical resistance. It is not affected by perspiration.
EUROPLEX® PPSU was tested by leading helmet and visor manufacturers. It obtained all necessary approvals in accordance to the ongoing standard EN 443:2008 for helmets for fire fighting in buildings and other structures and the integrated standard EN 14458:2004 for personal eye-equipment – face shields and visors for use with fire fighters - and high performance Industrial safety helmets used by fire fighters, ambulance and emergency services. The amber colored visors manufactured from EUROPLEX® PPSU can also be coated with anti-scratch or anti-fog surface layers. They can be supplied with or without a gold coating for applications with increased IR radiation.

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 70.0 - 80.0 MPa10200 - 11600 psiISO 527
Modulus of Elasticity 2.35 GPa341 ksiISO 527
Izod Impact, Notched (ISO) 50.0 - 60.0 kJ/m²23.8 - 28.6 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 190 °C374 °F
Vicat Softening Point 222 °C432 °FISO 306/B50

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone
Evonik Europlex® PPSU Polyphenylsulfone Engineering Plastic
IRPC Polimaxx Pentfoam 328H Expandable Polystyrene
Overview of materials for Polyphenylsulfone (PPSU)
RTP Company RTP Radel R-7700 Polyphenyl Sulfone (PPSU); Flame Retardant

PEVONIL152 / 196356

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.