MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion SupremEX® 215XK MMC Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ, Forged Plate
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy

Material Notes: SupremEX® 215XK MMC is a high quality, aerospace-grade aluminum alloy (2009) reinforced with 15 vol.% silicon carbide particles. This composite material is manufactured via powder metallurgy using a mechanical alloying process to ensure a homogeneous reinforcement distribution, providing a refined grain structure and enhancing mechanical properties. SupremEX 215XK is heat treatable, offering high strength and modulus for structural applications. It is available in billet, forged and extruded forms. Designation: – 2009/SiC/15p (5 µm).

Benefits

  • Weight saving versus titanium alloys
  • High fatigue and fretting fatigue resistance
  • Increased modulus versus aluminum alloys
  • Hardness, wear resistance and low friction characteristics
  • Good machinability using conventional techniques
  • Homogenous and stable microstructure

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.84 g/cc0.103 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 550 MPa79800 psi
Tensile Strength, Yield 385 MPa
@Strain 0.200 %
55800 psi
@Strain 0.200 %
Elongation at Break 8.00 %8.00 %
Modulus of Elasticity 94.0 GPa13600 ksi
Poissons Ratio 0.3000.300
Shear Modulus 36.0 GPa5220 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.5 µm/m-°C10.3 µin/in-°F
Specific Heat Capacity 0.848 J/g-°C0.203 BTU/lb-°F
Thermal Conductivity 155 W/m-K1080 BTU-in/hr-ft²-°F
Solidus 548 °C1020 °F
 
Descriptive Properties
Specific Stiffness33 GPa/g/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB9113d / 323536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.