MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Shawinigan Black® Acetylene Black ABBEADW  (discontinued **)
Categories: Carbon; Carbon Black

Material Notes: SHAWINIGAN ACETYLENE BLACK is made from acetylene gas and is the purest form of carbon black available. Its unique structural properties offer high liquid absorption, high electrical conductivity, and the ability to impart this conductivity into plastics, rubber, and other materials. This product is in beaded form. It is free flowing, less dusty, and easier to handle than flake products.

Moisture: 0.10% Typical; 0.5% Max. Ash: 0.005% Max. Average bead hardness (16-18 mesh) is typically 7.5 g with a minimum value of 6.0 g. Mass strength is typically 100 psi with a minimum value of 20 psi. DBPA No is typically 204 cc/100 g with a minimum of 180 cc/100 g. AWSR (500 mesh sieve) is < 20 ppm. pH is 7.0.

Data provided by Chevron Phillips Chemical Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³Typical
Apparent Bulk Density 0.270 g/cc0.00975 lb/in³Typical
Water Absorption 0.10 %0.10 %Typical
 <= 0.50 %<= 0.50 %
Particle Size 0.042 µm0.042 µmMean
pH 7.07.0
Specific Surface Area 70 m²/g70 m²/gBET Method
 
Component Elements PropertiesMetricEnglishComments
Carbon, C >= 99.9 %>= 99.9 %
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cancarb Thermax® Floform N990 Medium Thermal Carbon Black
Cancarb Thermax® Floform N990 Ultra-Pure Medium Thermal Carbon Black
Graphite, Carbon, C
Aremco Graphi-Bond™ 551-R
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled

E2CV05 / 3099

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.