MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Molding Grade

Material Notes: OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F without thermal degradation.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³ExxonMobil Method
Methyl Acrylate Content 16.5 %16.5 %
Melt Flow 0.70 g/10 min0.70 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 848415s; ASTM D2240
Hardness, Shore D 343415s; ASTM D2240
Tensile Strength at Break 12.1 MPa1750 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus, 1% Secant 57.2 MPa8300 psiASTM D790
Instrumented Impact Total Energy  20.3 J
@Temperature 23.0 °C
15.0 ft-lb
@Temperature 73.4 °F
ASTM D3763
 31.2 J
@Temperature -40.0 °C
23.0 ft-lb
@Temperature -40.0 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Melting Point 87.2 °C189 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 43.3 °C110 °FASTM D1525
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Arkema LOTRYL® 18 MA 02 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate
Dow Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating

PEXB171 / 37476

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.