MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plenco 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Heat Resistant Grade, Filled

Material Notes: Plaslok 506 is a two-stage, mineral-filled phenolic molding compound. It is formulated for automotive ashtrays and for appliance applications such as utensil handles receiving repeated exposure to 500°F. Plaslok 506 meets the following automotive specifications: Chrysler: MS-PP7-6, MS-DA43; Toyota: TSM6504AG-1; General Motors: CPC CMP PF002, APOPS 2401-01; Ford: ESB-M3D-118D, FMVSS 302

Data provided by Plaslok Corporation.

Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ASTM D792
Apparent Bulk Density 0.700 g/cc0.0253 lb/in³ASTM D1895
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inCompression; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 41.0 MPa5950 psiASTM D638
Flexural Yield Strength 69.0 MPa10000 psiASTM D790
Flexural Modulus 10.4 GPa1510 ksiASTM D790
Compressive Yield Strength 206 MPa29900 psiASTM D695
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM D257
Dielectric Constant  6.0
@Frequency 1e+6 Hz
6.0
@Frequency 1e+6 Hz
ASTM D150
 14
@Frequency 60 Hz
14
@Frequency 60 Hz
ASTM D150
Dielectric Strength 11.8 kV/mm300 kV/inASTM D149
Dissipation Factor  0.060
@Frequency 1e+6 Hz
0.060
@Frequency 1e+6 Hz
ASTM D150
 0.17
@Frequency 60 Hz
0.17
@Frequency 60 Hz
ASTM D150
Comparative Tracking Index 230 V230 VUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 182 °C360 °FASTM D648
UL RTI, Electrical 150 °C
@Thickness 1.57 mm
302 °F
@Thickness 0.0618 in
UL RTI, Mechanical with Impact 150 °C
@Thickness 1.57 mm
302 °F
@Thickness 0.0618 in
UL RTI, Mechanical without Impact 150 °C
@Thickness 1.57 mm
302 °F
@Thickness 0.0618 in
Flammability, UL94  V-0
@Thickness 1.57 mm
V-0
@Thickness 0.0618 in
 V-0
@Thickness 1.57 mm
V-0
@Thickness 0.0618 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plaslok 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
BASF Elastollan® C-60AW Polyester Type Polyurethane Elastomer
Plenco 6527 Phenolic, Granular, Transfer Molded
Arkema KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, 50% RH

PLEO909 / 50798

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.